MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Daplen™ EE015U TPO Compound  (discontinued **)
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Olefinic Elastomer (TPO); Polypropylene (PP); TPO

Material Notes: Daplen EE015U is a 10% mineral and elastomer modified polypropylene compound intended for injection molding. Daplen EE015U is a material with excellent impact /stiffness ratio. Thanks to its low thermal expansion this material is suitable to mold parts requiring low change of dimensions over a broad temperature range. This product is optimized to give good surface aesthetics.

Daplen EE015U has been developed especially for bumpers, spoilers and exterior trims.

Information provided by the Manufacturer.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.940 g/ccISO 1183
Linear Mold Shrinkage 0.0085 - 0.0095 cm/cmBorealis Method
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
ISO 1133
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 35.0 MPaAt 132 N/10 sec; ISO 2039
Tensile Strength, Yield 2393 psiAt 50 mm/min; ISO 527-2
Elongation at Break 100 %At 50 mm/min; ISO 527-2
Elongation at Yield 5.0 %At 50 mm/min; ISO 527-2
Tensile Modulus 1.15 GPaAt 1 mm/min; ISO 527-2
Flexural Strength 24.5 MPaISO 178
Flexural Modulus 1.15 GPaAt 2 mm/min; ISO 178
Charpy Impact Unnotched NBISO 179/1eU
 NB
@Temperature -20.0 °C
ISO 179/1eU
Charpy Impact, Notched 5.00 J/cm²ISO 179/1eA
 0.500 J/cm²
@Temperature -30.0 °C
ISO 179/1eA
 0.700 J/cm²
@Temperature -20.0 °C
ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear <= 85.0 µm/m-°C
@Temperature 100 °C
Borealis Test
Deflection Temperature at 0.46 MPa (66 psi) 89.0 °CISO 75-2
Deflection Temperature at 1.8 MPa (264 psi) 50.0 °CISO 75-2
Vicat Softening Point 47.0 °CB (50N); ISO 306
 132 °CA (10N); ISO 306
Shrinkage 0.15 %
@Temperature 90.0 °C,
Time 7200 sec
Post Shrinkage; Borealis Method
 
Processing PropertiesOriginal ValueComments
Melt Temperature 220 - 260 °CPolymer Mass Temp
Mold Temperature 30.0 - 50.0 °C

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Noble Polymers Regis™ 125098 Thermoplastic Olefin (TPO)
Borealis Daplen™ ED213AE TPO Compound
Borealis Daplen™ EE109AE TPO Compound
Borealis Daplen™ AK4504 TPO Compound
Borealis Daplen™ EH104AE Polypropylene TPO Compound

PBOREA148 / 27455

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.