H 203 is a high melt flow rate homopolymer with a general purpose additive package. This product exhibits excellent processability and good stiffness/impact strength balance. It also features a low taste/odor. It is designed for injection molding and fiber extrusion processing. Its applications include: injection of electric portables and household appliances; injected chest drawers and closets; continuous filaments for carpets, sewing threads, and ropes; staple fibers for rugs and blankets; and nonwovens by the thermobonded process. |