MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Haynes 556® alloy, 50% cold reduction
Categories: Metal; Superalloy; Iron Base

Material Notes: Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists corrosion by molten chloride salts and is resistant to corrosion from molten zinc. Excellent forming and welding characteristics. Applications include tubing and structural members in municipal and industrial waste incinerators, rotary calciners and kilns for minerals processing, and non-rotating components in land-based gas turbines burning low-grade fuels; carbon regenerators, and in processes involving high-sulfur petroleum feedstocks; widely used for hot-dip galvanizing fixtures, spinners, and baskets, high speed furnace fans, air preheaters of diesel engines, the inner covers of coil annealing furnaces, and various high temperature applications in the aerospace industry.

Data provided by the manufacturer, Haynes International, Inc.

Key Words: UNS R30556, AMS 5874, AMS 5877, AMS 5831
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Density 8.23 g/cc0.297 lb/in³at RT
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate 1410 MPa205000 psi
Tensile Strength, Yield 1170 MPa
@Strain 0.2 %
170000 psi
@Strain 0.2 %
Elongation at Break 8.0 %8.0 %in 50.8 mm
Modulus of Elasticity 205 GPa29700 ksiRT
 138 GPa
@Temperature 1000 °C
20000 ksi
@Temperature 1830 °F
 143 GPa
@Temperature 900 °C
20700 ksi
@Temperature 1650 °F
 148 GPa
@Temperature 800 °C
21500 ksi
@Temperature 1470 °F
 155 GPa
@Temperature 700 °C
22500 ksi
@Temperature 1290 °F
 164 GPa
@Temperature 600 °C
23800 ksi
@Temperature 1110 °F
 172 GPa
@Temperature 500 °C
24900 ksi
@Temperature 932 °F
 179 GPa
@Temperature 400 °C
26000 ksi
@Temperature 752 °F
 187 GPa
@Temperature 300 °C
27100 ksi
@Temperature 572 °F
 195 GPa
@Temperature 200 °C
28300 ksi
@Temperature 392 °F
 200 GPa
@Temperature 100 °C
29000 ksi
@Temperature 212 °F
Charpy Impact 240 J177 ft-lbSamples did not break. Average of 4 or more tests.
 
Electrical PropertiesMetricEnglishComments
Electrical Resistivity 0.0000952 ohm-cm0.0000952 ohm-cmRT
 0.0000986 ohm-cm
@Temperature 100 °C
0.0000986 ohm-cm
@Temperature 212 °F
 0.0001026 ohm-cm
@Temperature 200 °C
0.0001026 ohm-cm
@Temperature 392 °F
 0.0001065 ohm-cm
@Temperature 300 °C
0.0001065 ohm-cm
@Temperature 572 °F
 0.0001095 ohm-cm
@Temperature 400 °C
0.0001095 ohm-cm
@Temperature 752 °F
 0.0001125 ohm-cm
@Temperature 500 °C
0.0001125 ohm-cm
@Temperature 932 °F
 0.0001151 ohm-cm
@Temperature 600 °C
0.0001151 ohm-cm
@Temperature 1110 °F
 0.0001172 ohm-cm
@Temperature 700 °C
0.0001172 ohm-cm
@Temperature 1290 °F
 0.000119 ohm-cm
@Temperature 800 °C
0.000119 ohm-cm
@Temperature 1470 °F
 0.0001207 ohm-cm
@Temperature 900 °C
0.0001207 ohm-cm
@Temperature 1650 °F
 0.0001223 ohm-cm
@Temperature 1000 °C
0.0001223 ohm-cm
@Temperature 1830 °F
 0.0001237 ohm-cm
@Temperature 1100 °C
0.0001237 ohm-cm
@Temperature 2010 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear  14.7 µm/m-°C
@Temperature 25.0 - 100 °C
8.17 µin/in-°F
@Temperature 77.0 - 212 °F
 14.9 µm/m-°C
@Temperature 25.0 - 200 °C
8.28 µin/in-°F
@Temperature 77.0 - 392 °F
 15.1 µm/m-°C
@Temperature 25.0 - 300 °C
8.39 µin/in-°F
@Temperature 77.0 - 572 °F
 15.4 µm/m-°C
@Temperature 25.0 - 400 °C
8.56 µin/in-°F
@Temperature 77.0 - 752 °F
 15.7 µm/m-°C
@Temperature 25.0 - 500 °C
8.72 µin/in-°F
@Temperature 77.0 - 932 °F
 16.1 µm/m-°C
@Temperature 25.0 - 600 °C
8.94 µin/in-°F
@Temperature 77.0 - 1110 °F
 16.4 µm/m-°C
@Temperature 25.0 - 700 °C
9.11 µin/in-°F
@Temperature 77.0 - 1290 °F
 16.7 µm/m-°C
@Temperature 25.0 - 800 °C
9.28 µin/in-°F
@Temperature 77.0 - 1470 °F
 17.0 µm/m-°C
@Temperature 25.0 - 900 °C
9.44 µin/in-°F
@Temperature 77.0 - 1650 °F
 17.1 µm/m-°C
@Temperature 25.0 - 1000 °C
9.50 µin/in-°F
@Temperature 77.0 - 1830 °F
Specific Heat Capacity 0.464 J/g-°C0.111 BTU/lb-°FRT
 0.475 J/g-°C
@Temperature 100 °C
0.114 BTU/lb-°F
@Temperature 212 °F
 0.493 J/g-°C
@Temperature 200 °C
0.118 BTU/lb-°F
@Temperature 392 °F
 0.508 J/g-°C
@Temperature 300 °C
0.121 BTU/lb-°F
@Temperature 572 °F
 0.523 J/g-°C
@Temperature 400 °C
0.125 BTU/lb-°F
@Temperature 752 °F
 0.538 J/g-°C
@Temperature 500 °C
0.129 BTU/lb-°F
@Temperature 932 °F
 0.552 J/g-°C
@Temperature 600 °C
0.132 BTU/lb-°F
@Temperature 1110 °F
 0.561 J/g-°C
@Temperature 700 °C
0.134 BTU/lb-°F
@Temperature 1290 °F
 0.570 J/g-°C
@Temperature 800 °C
0.136 BTU/lb-°F
@Temperature 1470 °F
 0.595 J/g-°C
@Temperature 900 °C
0.142 BTU/lb-°F
@Temperature 1650 °F
 0.618 J/g-°C
@Temperature 1000 °C
0.148 BTU/lb-°F
@Temperature 1830 °F
 0.638 J/g-°C
@Temperature 1100 °C
0.152 BTU/lb-°F
@Temperature 2010 °F
Thermal Conductivity 11.1 W/m-K77.0 BTU-in/hr-ft²-°FRT
 13.1 W/m-K
@Temperature 100 °C
90.9 BTU-in/hr-ft²-°F
@Temperature 212 °F
 15.4 W/m-K
@Temperature 200 °C
107 BTU-in/hr-ft²-°F
@Temperature 392 °F
 17.3 W/m-K
@Temperature 300 °C
120 BTU-in/hr-ft²-°F
@Temperature 572 °F
 19.0 W/m-K
@Temperature 400 °C
132 BTU-in/hr-ft²-°F
@Temperature 752 °F
 20.8 W/m-K
@Temperature 500 °C
144 BTU-in/hr-ft²-°F
@Temperature 932 °F
 22.4 W/m-K
@Temperature 600 °C
155 BTU-in/hr-ft²-°F
@Temperature 1110 °F
 24.0 W/m-K
@Temperature 700 °C
167 BTU-in/hr-ft²-°F
@Temperature 1290 °F
 25.5 W/m-K
@Temperature 800 °C
177 BTU-in/hr-ft²-°F
@Temperature 1470 °F
 27.2 W/m-K
@Temperature 900 °C
189 BTU-in/hr-ft²-°F
@Temperature 1650 °F
 28.9 W/m-K
@Temperature 1000 °C
201 BTU-in/hr-ft²-°F
@Temperature 1830 °F
 30.4 W/m-K
@Temperature 1100 °C
211 BTU-in/hr-ft²-°F
@Temperature 2010 °F
Melting Point 1330 - 1415 °C2430 - 2579 °F
Solidus 1330 °C2430 °F
Liquidus 1415 °C2579 °F
 
Component Elements PropertiesMetricEnglishComments
Aluminum, Al 0.20 %0.20 %
Carbon, C 0.10 %0.10 %
Chromium, Cr 22 %22 %
Cobalt, Co 18 %18 %
Iron, Fe 31 %31 %As remainder
Lanthanum, La 0.020 %0.020 %
Manganese, Mn 1.0 %1.0 %
Molybdenum, Mo 3.0 %3.0 %
Nickel, Ni 20 %20 %
Nitrogen, N 0.20 %0.20 %
Silicon, Si 0.40 %0.40 %
Tantalum, Ta 0.60 %0.60 %
Tungsten, W 2.5 %2.5 %
Zirconium, Zr 0.020 %0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Haynes Alloy No. 151 cast Superalloy
Haynes 556® alloy, 0% cold reduction
Haynes 282® Nickel Alloy Sheet, Plate and Bar, Solution Annealed
Haynes 263® alloy, cold rolled sheet, solution treated and aged
Haynes 25 alloy, sheet

NH55BL / 16692

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.