MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Schott N-SF4 Glass
Categories: Ceramic; Glass

Material Notes:

Information Provided by SCHOTT North America, Inc.

Key Words: 755274.315
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 3.15 g/cc0.114 lb/in³
 
Chemical PropertiesMetricEnglishComments
Acid Class, SR 1.31.3
Alkali Class, AR 1.01.0
Stain Resistance Class, FR 0.000.00
 
Mechanical PropertiesMetricEnglishComments
Knoop Microhardness 520520.1/20
Modulus of Elasticity 90.0 GPa13100 ksi
Poissons Ratio 0.2560.256
Shear Modulus 36.0 GPa5220 ksicalculated
 
Thermal PropertiesMetricEnglishComments
CTE, linear  9.50 µm/m-°C
@Temperature -30.0 - 70.0 °C
5.28 µin/in-°F
@Temperature -22.0 - 158 °F
 10.9 µm/m-°C
@Temperature 20.0 - 300 °C
6.06 µin/in-°F
@Temperature 68.0 - 572 °F
Specific Heat Capacity 0.760 J/g-°C0.182 BTU/lb-°F
Thermal Conductivity 0.950 W/m-K6.59 BTU-in/hr-ft²-°F
Transformation Temperature, Tg 570 °C1060 °F
Softening Point 661 °C1220 °FViscosity 107.6 dPa s
Annealing Point 559 °C1040 °FViscosity 1013.0 dPa s
 
Optical PropertiesMetricEnglishComments
Refractive Index  1.75513
@Wavelength 587.6 nm
1.75513
@Wavelength 587.6 nm
nd
 1.76164
@Wavelength 546.1 nm
1.76164
@Wavelength 546.1 nm
ne
Abbe Number 27.1627.16ve
 27.3827.38vd
Optical Dispersion 0.0275830.027583nf - nc
 0.0280440.028044nf' - nc'
Transmission, Visible  45.5 %
@Thickness 10.0 mm,
Wavelength 380 nm
45.5 %
@Thickness 0.394 in,
Wavelength 380 nm
 82.1 %
@Thickness 10.0 mm,
Wavelength 405 nm
82.1 %
@Thickness 0.394 in,
Wavelength 405 nm
 95.9 %
@Thickness 10.0 mm,
Wavelength 460 nm
95.9 %
@Thickness 0.394 in,
Wavelength 460 nm
 99.3 %
@Thickness 10.0 mm,
Wavelength 580 nm
99.3 %
@Thickness 0.394 in,
Wavelength 580 nm
 99.5 %
@Thickness 10.0 mm,
Wavelength 700 nm
99.5 %
@Thickness 0.394 in,
Wavelength 700 nm
IR Transmittance  90.1 %
@Thickness 10.0 mm,
Wavelength 2500 nm
90.1 %
@Thickness 0.394 in,
Wavelength 2500 nm
 99.7 %
@Thickness 10.0 mm,
Wavelength 1530 nm
99.7 %
@Thickness 0.394 in,
Wavelength 1530 nm
UV Transmittance  4.4 %
@Thickness 10.0 mm,
Wavelength 365 nm
4.4 %
@Thickness 0.394 in,
Wavelength 365 nm
 15.2 %
@Thickness 10.0 mm,
Wavelength 370 nm
15.2 %
@Thickness 0.394 in,
Wavelength 370 nm
 
Descriptive Properties
B1
Climatic Resistance Test CR1
HG6
K (10-6mm2/N)2.76
Phosphate Resistance PR1

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Ohara S-PHM52 Optical Glass
Schott LG-680 Silicate Laser Glass
Schott N-SF2 Glass
Schott N-SF15 Glass
Schott N-SF14 Glass

CSGS071 / 93405

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.