MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Teknor Apex Sinvicomp SIZ5305 Flexible Polyvinyl Chloride
Categories: Polymer; Thermoplastic; Vinyl (PVC); PVC, Flexible Grade

Material Notes: Sinvicomp SIZ5305 is a wire & cable polyvinylchloride compound available in pellet form. It provides good performance for insulation of electrical wires.

Availability: Asia Pacific

Features: High Stiffness

Uses: Insulation

Agency Rating: IEC 60227

RoHS Compliant:RoHS Compliant

Form: Pellets

Processing Method: Extrusion

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.45 g/cc0.0524 lb/in³ASTM D792
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 9191ASTM D2240
Tensile Strength, Yield 16.0 MPa2320 psiIEC 60811-1-1
 17.6 MPa
@Treatment Temp. 136 °C,
Time 864000 sec
2550 psi
@Treatment Temp. 277 °F,
Time 240 hour
Change After Aging in Air Oven; IEC 811-1-2
Elongation at Break 250 %250 %IEC 60811-1-1
 288 %
@Treatment Temp. 136 °C,
Time 864000 sec
288 %
@Treatment Temp. 277 °F,
Time 240 hour
Change After Aging in Air Oven; IEC 811-1-2
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity 1.00e+14 ohm-cm1.00e+14 ohm-cmBS 2782
 
Processing PropertiesMetricEnglishComments
Processing Temperature 170 - 180 °C338 - 356 °FCompression Zone
 175 - 185 °C347 - 365 °FMixing Zone
Feed Temperature 160 °C320 °F
Nozzle Temperature 185 °C365 °F
 
Descriptive Properties
Heat Stability3.5 hr(392°F), BS 2782

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTEKNQ1499 / 237990

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.