MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK Laponite® ED Silicate
Categories: Ceramic; Clay; Other Engineering Material; Additive/Filler for Polymer

Material Notes: Laponite® ED is a layered silicate with very low heavy metals content. It has been specially designed for addition directly into the organic phase during preparation of a range of oil-in-water emulsion systems. This novel procedure with Laponite® ED can result in a significant reduction in the time required to make stable emulsion systems.

Information provided by Southern Clay Products

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 62.4 lb/ft³
Particle Mesh Size >= 250 Mesh<1%
pH 9.82% suspension
Specific Surface Area 370 m²/g
 
Processing PropertiesOriginal ValueComments
Gel Time 22.0 ming
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 10 %Free
Loss on Ignition(%) 8.2 %
MgO 27.5 %
Na2O 2.8 %
SiO2 59.5 %
 
Descriptive Properties
Color/FormFree flowing white powder
Composition>1 mg/kgArsenic
 >5 mg/kgLead
 0.008Li2O

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BYK Laponite® S Synthetic Layered Fluorosilicate
BYK Laponite® RDS Synthetic Layered Silicate
BYK Laponite® RD Synthetic Layered Silicate
BYK Laponite® OG Clay Additive
BYK Laponite® LV Clay Additive

PBYK060 / 185057

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.