System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
Envalior Durethan® BM 40 X H2.0 EF 900116 Nylon 6 (PA6), 40% Glass/Mineral Filled, Dry
Categories:
Polymer
;
Thermoplastic
;
Nylon (Polyamide PA)
;
Nylon 6 (PA6)
;
Nylon 6, Glass/Mineral Reinforced
Material Notes:
PA 6, 40% glass fibers/mineral, injection molding, improved flowability, heat-aging stabilized, low tendency to warp, improved surface finish
Former Lanxess product line is now with Envalior.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Metric
English
Comments
Bulk Density
0.700
g/cc
0.0253
lb/in³
ISO 60
Density
1.45
g/cc
0.0524
lb/in³
ISO 1183
Linear Mold Shrinkage, Flow
0.0025
cm/cm
0.0025
in/in
150x105x3; 290 °C / MT 80 °C; 500 bar; ISO 294-4
0.0072
cm/cm
0.0072
in/in
60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
Linear Mold Shrinkage, Transverse
0.0072
cm/cm
0.0072
in/in
60x60x2; 290 °C / MT 80°C; 600 bar; ISO 294-4
0.0087
cm/cm
0.0087
in/in
150x105x3; 290 °C / MT 80 °C; 500 bar; ISO 294-4
Mechanical Properties
Metric
English
Comments
Ball Indentation Hardness
210
MPa
30500
psi
ISO 2093-1
Tensile Strength at Break
125
MPa
18100
psi
5 mm/min; ISO 527-1,-2
Elongation at Break
2.5 %
2.5 %
5 mm/min; ISO 527-1,-2
Tensile Modulus
9.00
GPa
1310
ksi
1 mm/min; ISO 527-1,-2
Flexural Strength
206
MPa
29900
psi
2 mm/min; ISO 178-A
Flexural Yield Strength
200
MPa
@Strain 3.5 %
29000
psi
@Strain 3.5 %
2 mm/min; ISO 178-A
Flexural Modulus
8.80
GPa
1280
ksi
2 mm/min; ISO 178-A
Flexural Strain at Break
2.9 %
2.9 %
2 mm/min; ISO 178-A
Izod Impact, Notched (ISO)
<=
10.0
kJ/m²
@Temperature 23.0 °C
<=
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1A
<=
10.0
kJ/m²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1A
Izod Impact, Unnotched (ISO)
33.0
kJ/m²
@Temperature -30.0 °C
15.7
ft-lb/in²
@Temperature -22.0 °F
ISO 180-1U
35.0
kJ/m²
@Temperature 23.0 °C
16.7
ft-lb/in²
@Temperature 73.4 °F
ISO 180-1U
Charpy Impact Unnotched
4.00
J/cm²
@Temperature 23.0 °C
19.0
ft-lb/in²
@Temperature 73.4 °F
ISO 179-1eU
6.50
J/cm²
@Temperature -30.0 °C
30.9
ft-lb/in²
@Temperature -22.0 °F
ISO 179-1eU
Charpy Impact, Notched
<=
1.00
J/cm²
@Temperature 23.0 °C
<=
4.76
ft-lb/in²
@Temperature 73.4 °F
ISO 179 1eA
<=
1.00
J/cm²
@Temperature -30.0 °C
<=
4.76
ft-lb/in²
@Temperature -22.0 °F
ISO 179 1eA
Thermal Properties
Metric
English
Comments
CTE, linear, Parallel to Flow
28.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
15.6
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
CTE, linear, Transverse to Flow
85.0
µm/m-°C
@Temperature 23.0 - 55.0 °C
47.2
µin/in-°F
@Temperature 73.4 - 131 °F
ISO 11359-1,-2
Melting Point
220
°C
428
°F
10°C/min; ISO 11357-1,-3
Deflection Temperature at 0.46 MPa (66 psi)
215
°C
419
°F
ISO 75-1,-2
Deflection Temperature at 1.8 MPa (264 psi)
195
°C
383
°F
ISO 75-1,-2
Flammability, UL94
HB
@Thickness 1.60 mm
HB
@Thickness 0.0630 in
HB
@Thickness 0.800 mm
HB
@Thickness 0.0315 in
Shrinkage, MD
0.050 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.050 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction; 60x60x2; ISO 294-4
0.050 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.050 %
@Treatment Temp. 248 °F,
Time 4.00 hour
Post-Shrinkage Flow Direction 150x105x3; ISO 294-4
Shrinkage, TD
0.11 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.11 %
@Treatment Temp. 248 °F,
Time 4.00 hour
60x60x2; ISO 294-4
0.15 %
@Treatment Temp. 120 °C,
Time 14400 sec
0.15 %
@Treatment Temp. 248 °F,
Time 4.00 hour
150x105x3; ISO 294-4
Processing Properties
Metric
English
Comments
Melt Temperature
290
°C
554
°F
injection molding
280
-
300
°C
536
-
572
°F
Mold Temperature
80.0
°C
176
°F
injection molding
80.0
-
100
°C
176
-
212
°F
Drying Temperature
80.0
°C
176
°F
Dry Time
2.00
-
6.00
hour
2.00
-
6.00
hour
Moisture Content
0.030 - 0.12 %
0.030 - 0.12 %
Karl Fischer
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to view all the property values for this datasheet as they were originally entered into MatWeb.
Users viewing this material also viewed the following:
Eurotec® Tecomid® NB40 KK40 NL PA6, 40% glass fiber/mineral reinforced, natural
Envalior Durethan® BM 40 X H3.0 EF 000000 Nylon 6 (PA6), 40% Glass/Mineral Filled, Dry
Envalior Durethan® BM 40 X H2.0 EF 900116 Nylon 6 (PA6), 40% Glass/Mineral Filled, Conditioned
Envalior Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Dry
Envalior Durethan® BM 40 X H2.0 DUS009 901510 Nylon 6 (PA6), 40% Glass/Mineral Reinforced, Conditioned
PLANW9454 / 208291
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.