MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Shanghai Potomer CSM 40M Chlorosulfonated Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: Applications: The applications concern the greater part of industry as for instance the automotive, electric, house building, cables, and rolls. The most common manufactured articles are:
  • pipes for the transport of inorganic aggressive chemical solution
  • insulation cover
  • membranes of waterproofing for roofs, reservoirs, basins
  • conveyors belt for mineral

    Information provided by Shanghai Potomer International Trade Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Volatiles <= 1.5 %<= 1.5 %
Mooney Viscosity 40 - 60
@Temperature 100 °C
40 - 60
@Temperature 212 °F
ML 1+4
 
Mechanical PropertiesMetricEnglishComments
Tensile Strength >= 25.0 MPa>= 3630 psi
Elongation at Break >= 450 %>= 450 %
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 33 - 37 %33 - 37 %
Sulfur, S 0.80 - 1.2 %0.80 - 1.2 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSPOTOM053 / 284499

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.