MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Lord Adhesives 5181 High Viscosity, Black, General Purpose Ethyl Cyanoacrylate Adhesive
Categories: Polymer; Adhesive; Thermoset; Acrylic/Cyanoacrylate Adhesive

Material Notes:
Lord Cyanoacrylate Adhesives
Lord® Cyanoacrylate Adhesives were developed for production situations requiring instant bonds and immediate handling strength, particularly when bonding rubber, metals and plastics. Lord Cyanoacrylate Adhesives offer these benefits: Instant Cure. Lord Cyanoacrylate Adhesives develop strong bonds with setting times ranging from 5 to 130 seconds. Ease of Use. Lord Cyanoacrylate Adhesives are one-component systems that facilitate set-up and minimize production costs. Good Environmental Resistance. Lord Cyanoacrylate Adhesives offer excellent resistance to weathering and aging.

Lord Adhesives 5181 High Viscosity, Black, General Purpose Ethyl Cyanoacrylate Adhesive
High viscosity. Black general purpose adhesive. Suitable for bonding porous substrates and materials with different coefficients of thermal expansion. Repositioning of parts and inspection of bonded assemblies is also possible. Especially useful in loudspeaker assembly. Resists temperatures to 250°F (121°C).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.09 g/cc0.0393 lb/in³
Viscosity 2400 cP2400 cP
 
Processing PropertiesMetricEnglishComments
Cure Time 0.500 - 0.583 min0.00833 - 0.00972 hourPlastic set time
 0.500 - 0.583 min0.00833 - 0.00972 hourRubber set time
 1.33 - 2.00 min0.0222 - 0.0333 hourMetal set time

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
LATI LASTIROL R G/30 30% Glass Fiber Reinforced Polystyrene (PS)
LATI Kelon® A FR H2 CETG/300-V0 PA 66, Glass/Mineral Reinforced, Flame Retardant, Heat Stabilized
Atom Adhesives AA-BOND 2156 Epoxy Adhesive

PLORDAD56 / 52038

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.