MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Morgan Advanced Ceramics Superwool® Blanket HT Thermal Ceramic
Categories: Ceramic; Oxide

Material Notes: Superwool ® Plus and Superwool ® HT blanket offer the same benefits as the other members of the Superwool fiber family but with improved handling strength and enhanced thermal properties. Superwool ® Plus and Superwool ® HT blanket are manufactured from pure raw materials using a new manufacturing technology. In addition to enhanced thermal properties, large nuisance dust particles have been effectively eliminated making the product soft to the touch and less irritating during use.

Typical applications:

  • Power generation especially HRSG duct insulation
  • Chimney insulation
  • Process heater linings
  • Pipe wrap
  • Annealing furnace linings
  • Furnace and kiln back-up insulation
  • Storage heater insulation
  • Domestic oven insulation
  • Automotive exhaust heat shields
  • Aluminium transfer launder covers
  • Welding stress relief

Information provided by Morgan Advanced Materials

Key Words: Thermal Ceramics
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.0640 g/cc
 0.0960 g/cc
 0.128 g/cc
 0.160 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 0.0300 MPaat 64kg/m3; EN 1094-1
 0.0500 MPaat 96kg/m3; EN 1094-1
 0.0750 MPaat 128 kg/m3; EN 1094-1
 0.0950 MPaat 160 kg/m3; EN 1094-1
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0400 W/m-K
@Temperature 200 °C
at 128kg/m3
 0.0500 W/m-K
@Temperature 200 °C
at 96 kg/m3
 0.0800 W/m-K
@Temperature 400 °C
at 128kg/m3
 0.100 W/m-K
@Temperature 400 °C
at 96 kg/m3
 0.140 W/m-K
@Temperature 600 °C
at 128kg/m3
 0.190 W/m-K
@Temperature 600 °C
at 96 kg/m3
 0.230 W/m-K
@Temperature 800 °C
at 128kg/m3
 0.320 W/m-K
@Temperature 800 °C
at 96 kg/m3
 0.340 W/m-K
@Temperature 1000 °C
at 128kg/m3
 0.480 W/m-K
@Temperature 1200 °C
at 128kg/m3
 0.480 W/m-K
@Temperature 1000 °C
at 96 kg/m3
 0.690 W/m-K
@Temperature 1200 °C
at 96 kg/m3
 
Component Elements PropertiesOriginal ValueComments
CaO+MgO 18 - 25 %
Other <= 3.0 %oxides
SiO2 70 - 80 %
 
Descriptive Properties
Classification Temperature (°C)1300
Colorwhite

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Morgan Advanced Ceramics Ceramic Fiber Board S Board Ceramic Fibre Board
Thermal Ceramics Alfibond 2100 Shapes
Morgan Advanced Ceramics Ceramic Fiber Ropes Twisted Ceramic Fiber
Morgan Advanced Ceramics Ceramic Fiber Blankets Cerawool Blanket
Morgan Advanced Ceramics Ceraform 250 Ceramic Fiber

CMORF70105 / 203403

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.