N48 is an iron-nickel controlled expansion alloy suitable to soft glass sealing, with optimal chemical composition to obtain hermetic seals. Typical applications are hermetic feed throughs and electron gun components. International standards: ASTM F30 - DIN 17745 - W 1.3922 - A54-301 Information provided by Aperam |