MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Avient PolyOne® 2116 Black PEC Black Polyethylene  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polyethylene (PE)

Material Notes:

This concentrate has been designed for in-plant blending with appropriate natural high density polyethylene pipe resins to produce pipe with PE 2406 or PE 3408 ratings. 2116 Black PEC is manufactured to produce pipe free of surface imperfections with minimum screen pack plugging during extrusion. The carrier resin and stabilization system has been selected to maximize the physical and environmental properties of the pipe. A furnace carbon black has been selected to maximize processibility, while providing good outdoor weathering capability.

Description/Features:

  • Exterior-Weatherable
  • Black

Applications:

  • Pipe-Pressure
  • Pipe Fittings
  • Pipe Coupling

Processing Method:

  • Extrusion and Molding

Note: In order to meet requirements of the Plastics Pipe Institute (PPI), the pressure performance of pipe extruded from these blends must be verified. In-plant blending conditions and quality control procedures are important to achieve quality product, which will continue to meet these conditions. 2116 Black PEC is designed to be used at a 6.5% letdown rate in PPI TR-4 listed blends.

Information provided by PolyOne Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Carbon Black Loading 35 %
High Load Melt Index 20 g/10 min
@Load 21.6 kg,
Temperature 190 °C
Procedure A - Manual Operation; ASTM D1238
 
Descriptive Properties
CarrierLinear Medium Density Polyethylene
Product FormUnderwater Cut Pellets

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Axiall 19920 Wire & Cable Flexible PVC
Axiall 19900 Wire & Cable Flexible PVC
Axiall 19854 Wire & Cable Flexible PVC
Overview of materials for PVC, Wire and Cable Grade
Overview of materials for PVC, Uncompounded

PH1PO3396 / 45056

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.