MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Westlake LF 1050CC LLDPE, Butene Film Grade  (discontinued **)
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Film Grade; LLDPE/Butene, Film

Material Notes: LF1050 is a butene LLDPE with high stiffness suitable for cast film extrusion. This material can be used at 100% or as blending stock with LDPE or mPE. Test specimens for cast film: nominal thickness 1.0 mils; 13 lbs/die inch @ 525° F melt temperature and 70° F chill roll temperature. This product has some 21 CFR clearances. Application/Uses: Cast Film Extrusion- Profile Cast Film- Blend resin for GP Packaging.

Samples tested at 23°C and 50% RH.

Information provided by Westlake Chemical Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.925 g/cc0.0334 lb/in³ASTM D1505
Thickness 25.4 microns1.00 milCast Film as Tested
Melt Index of Compound 3.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
3.5 g/10 min
@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
 
Mechanical PropertiesMetricEnglishComments
Film Tensile Strength at Yield, MD 11.7 MPa1700 psiASTM D882
Film Tensile Strength at Yield, TD 12.4 MPa1800 psiASTM D882
Film Elongation at Break, MD 700 %700 %ASTM D882
Film Elongation at Break, TD 800 %800 %ASTM D882
Impact 9090grams; ASTM D1709A
Elmendorf Tear Strength, MD 2.36 g/micron
@Thickness 0.0254 mm
60.0 g/mil
@Thickness 0.00100 in
ASTM D1922
Elmendorf Tear Strength, TD 11.8 g/micron
@Thickness 0.0254 mm
300 g/mil
@Thickness 0.00100 in
ASTM D1922
Film Tensile Strength at Break, MD 32.4 MPa4700 psiASTM D882
Film Tensile Strength at Break, TD 21.4 MPa3100 psiASTM D882
1% Secant Modulus, MD 214 MPa31000 psiASTM D882
1% Secant Modulus, TD 248 MPa36000 psiASTM D882
 
Optical PropertiesMetricEnglishComments
Haze 2.0 %2.0 %no antiblock; ASTM D1003
Gloss 90 %90 %@ 45°, no antiblock, cast; ASTM D2457
 
Processing PropertiesMetricEnglishComments
Melt Temperature 260 - 288 °C500 - 550 °Fcast melt
 
Compliance PropertiesMetricEnglishComments
FDA YesYesSee notes for details.

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PWESF8824 / 222896

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.