MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Kennametal Stellite Stellite® 25 Cobalt Chromium Cast Alloy
Categories: Metal; Nonferrous Metal; Cobalt Alloy; Superalloy

Material Notes: Stellite alloy 25 forms a protective oxide film during hot metal-on metal wear which prevents metal transfer and damage due to adhesion. The alloy is resistant to thermal cracking and surface fatigue. Since the micro-structure is relatively free of carbide reinforcement, it is not recommended for low stress or low angle particle erosion service.

Stellite alloy 25 is resistant to oxidation and carburization up to 1900°F. The alloy resists wet chlorine at ambient temperatures and is resistant to nitric and hydrochloric acids under certain conditions. Exposure testing is recommended to verify performance.

Applications include metal working tools where a combination of metal-on-metal wear, thermal fatigue and hot corrosion resistance are required, such as piercing points, forming tools, and extrusion dies. Also used for furnace hardware. The alloy is normally used in the as-cast condition, but can be age hardened in the 1300° to 1500°F range for 4 to 50 hours. Solution annealing involves quenching or forced air cooling from 2175° to 2225°F.

Information provided by Deloro Stellite Inc.

Product of former Deloro Stellite Inc.

Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.31 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Brinell 350
 130
@Temperature 900 °C
 280
@Temperature 500 °C
Hardness, Rockwell C 10 - 35
Tensile Strength, Ultimate 925 MPa
Tensile Strength, Yield 895 MPa
Elongation at Break 5.0 %
Reduction of Area 7.0 %
Modulus of Elasticity 207 GPa
Charpy Impact 8.70 JV Notch
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.9 µm/m-°C
@Temperature 20.0 - 205 °C
 14.4 µm/m-°C
@Temperature 20.0 - 538 °C
 14.8 µm/m-°C
@Temperature 20.0 - 650 °C
 16.2 µm/m-°C
@Temperature 20.0 - 877 °C
 16.9 µm/m-°C
@Temperature 20.0 - 982 °C
Thermal Conductivity 9.40 W/m-K
Melting Point 1329 - 1410 °C
Solidus 1329 °C
Liquidus 1410 °C
Maximum Service Temperature, Air 1038 °COxidation resistant
 
Component Elements PropertiesOriginal ValueComments
Boron, B 0.00 %
Carbon, C <= 0.45 %
Chromium, Cr 20 %
Cobalt, Co 51 %As remainder
Iron, Fe 2.0 %
Manganese, Mn 1.5 %
Nickel, Ni 10 %
Silicon, Si 0.70 %
Tungsten, W 15 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kennametal Stellite Stellite® 21
Kennametal Stellite Stellite® 4 Cobalt Chromium Alloy
Kennametal Stellite Deloro® 716 PM cast
Kennametal Stellite Deloro® 711 PM cast
Kennametal Stellite Stellite® 98M2 cast

NS25 / 18860

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.