MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

(Viewing data as-entered. Click here to return)
Lehmann & Voss LUVOCOM® 1114-0717 PAEK with carbon fiber and PTFE
Categories: Polymer; Thermoplastic; Polyketone; Polyaryletherketone (PAEK), Carbon Fiber Filled

Material Notes: Properties/attributes include: Good friction and wear behavior especially at high temperatures. Electrically conductive, suitable for continuous discharging of statically-generated electricity.

Automotive industry, textile machinery, medical- and precision engineering, aircraft industry. Typical uses include: Thermic, mechanic and chemical highly stressed parts.

Processing: During processing, the moisture content should not exceed 0.05%. To avoid internal stresses, a medium to high injection rate should be used. An increase in tool temperature may be helpful. Post-crystallization may lead to warpage at elevated operating temperatures. This can be counteracted by suitable heat treatment. The processing notes provided merely represent a recommendation for general use. Due to the large variety of machines, geometries and volumes of parts, etc., it may be necessary to employ different settings according to the specific application. High-temperature polymers place increased demands on the tool steels employed.

Information provided by Lehmann & Voss & Co.KG

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.51 g/ccISO 1183
Moisture Absorption <= 0.100 %
@Temperature 23.0 °C,
Time 86400 sec
Linear Mold Shrinkage 0.0010 - 0.0030 cm/cmDIN 16901
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 180 MPaISO 527-2
Elongation at Break 1.5 %ISO 527-2
Modulus of Elasticity 17.0 GPaISO 527-2
Flexural Strength 240 MPaISO 178
Flexural Modulus 14.0 GPaISO 178
Flexural Strain at Break 2.0 %Flexural Elongation @ Fmax; ISO 178
Charpy Impact Unnotched 20.0 kJ/m²
@Temperature -30.0 °C
ISO 179
 25.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1fu
Charpy Impact, Notched 12.0 kJ/m²
@Temperature 23.0 °C
ISO 179 1eA
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity <= 1e+05IEC 60167
Surface Resistance <= 10000 ohmIEC 60093
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 µm/m-°CDIN 53752
Thermal Conductivity 0.600 W/m-KDIN 52612
Maximum Service Temperature, Air 255 °CContinuous; UL 746B
Deflection Temperature at 1.8 MPa (264 psi) 305 °CISO 75-2/A
Vicat Softening Point 320 °CVST A; DIN ISO 306
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 390 - 420 °C
Zone 1 370 - 420 °C
Zone 2 380 - 420 °C
Zone 3 390 - 420 °C
Melt Temperature 390 °C
Mold Temperature 160 - 200 °C
Drying Temperature 120 °C
@Time 21600 - 36000 sec
Dehumidifying dryer
 150 °C
@Time 14400 - 21600 sec
Dehumidifying dryer
Moisture Content <= 0.050 %
 
Descriptive Properties
Colordark grey

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Lehmann & Voss LUVOCOM® 1200-7116-1 ABS with carbon fiber
Gharda Chemicals GATONE™ 5330CF Polyetheretherketone (PEEK)

PLUU8864 / 193823

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.