MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt SILVALOY® 999 (BRAZE™ 999) >99.95% Silver (AWS BVAg-0 Grade 2)
Categories: Metal; Nonferrous Metal; Precious Metal; Silver Alloy; Solder/Braze Alloy; Pure Element

Material Notes: Silvaloy 999 is widely used in numerous electrical, electronic, and industrial applications such as contacts, fuse elements, lead wires, battery plated and ruptured discs. Fine silver is generally selected for its high thermal and electrical conductivity, as well as for its good resistance to oxidation and corrosive attack. It also exhibits excellent ductility and is easily joined by welding or brazing. Silvaloy 999 is also used to join metalized ceramics in reducing or inert atmospheres or vacuum. Silvaloy 999, as a pure metal, melts and flows at a single temperature, meaning it will flow quickly and fill tight clearances well. While Silvaloy 999 will wet most ferrous and nonferrous surfaces, excessive hold time at braze temperature should be avoided to lessen the possibility of diffusion into the base metal, especially on copper alloys.

Available forms: Wire, strip, engineered preforms, and specialty preforms.

Information provided by Lucas-Milhaupt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.379 lb/in³
Vapor Pressure 0.00130 atm
@Temperature 1360 °C
 
Chemical PropertiesOriginal ValueComments
Atomic Mass 107.9
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000164 ohm-cm
@Temperature 20.0 °C
varies according to temper and purity
 
Thermal PropertiesOriginal ValueComments
CTE, linear 19.0 µm/m-°C
@Temperature 100 °C
Specific Heat Capacity 0.0560 BTU/lb-°F
@Temperature 20.0 °C
Thermal Conductivity 1.00 cal cm/sec-cm²-°C
@Temperature 20.0 °C
Melting Point >= 1761 °F
Solidus 1761 °F
Boiling Point 4010 °F
 
Component Elements PropertiesOriginal ValueComments
Cadmium, Cd <= 0.0020 %
Carbon, C <= 0.0050 %
Copper, Cu <= 0.050 %
Lead, Pb <= 0.0020 %
Other, each <= 0.0020 %High vapor pressure elements.
Other, total <= 0.010 %high vapor pressure elements (Including zinc, cadmium, and lead)
Phosphorus, P <= 0.0020 %
Silver, Ag >= 99.95 %
Zinc, Zn <= 0.0020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCM9845 / 254790

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.