Hostacom ERS 5011L G35996 is an unfilled copolymer with high melt flow rate. Product is UL certified. Availability: Asia-Pacific Application: White Goods Market: Electrical / Electronics Processing Method: Injection Molding Information provided by LyondellBasell. |