MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Aremco

Aremco EZ-Cast™ 580N Silicon Molding Compound Silicone Rubber
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE); Silicone

Material Notes: Aremco's EZ-Cast™ 580N is an ideal compound for producing high reliability master molds. This silicone rubber compound exhibits high tear strength, very low shrinkage and high flexibility, all requirements for detailed reproduction.

Vendors: Aremco’s Ceramacast casting and potting compounds represent the most expansive line of products based on aluminum oxide, aluminum nitride, magnesium oxide, silicon dioxide, silicon carbide, zirconium oxide, and zirconium silicate for applications to 3000°F (1760°C). Visit us today at Aremco.com or call 1 (845) 268-0039 to speak with an engineer.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.30 g/cc1.30 g/cc
Viscosity 30000 cP30000 cPMixed
Linear Mold Shrinkage <= 0.0010 cm/cm<= 0.0010 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 4545Durometer
Tensile Strength at Break >= 4.14 MPa>= 600 psi
Elongation at Break >= 400 %>= 400 %
Tear Strength >= 19.3 kN/m>= 110 pliDie B
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 204 °C400 °F
Minimum Service Temperature, Air -60.0 °C-76.0 °F
 
Processing PropertiesMetricEnglishComments
Pot Life 30 min30 min
Shelf Life 6.00 Month6.00 Month
 
Descriptive Properties
ColorBeige Resin; Deep Red Catalyst
Mix Ratio by Weight10:1resin:catalyst

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Overview of materials for Silicone Rubber
Overview of materials for Liquid Silicone Rubber
Abatron L060421-1 Heat-Resistant Non-Flammable Silicone Rubber
Rogers Arlon CP-375CR Silicone Rubber
Rogers Arlon CP-510R Silicone Rubber

PAREM41 / 24305

Free Trade Publications, Click Here!
Free Trade Publications, Click Here!

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.