MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Celanese Zenite® ZE55801 NC010 LCP
Categories: Polymer; Thermoplastic; Liquid Crystal Polymer (LCP); Liquid Crystal Polymer (LCP), 30% Glass Fiber Filled

Material Notes: Zenite® ZE55801 NC010 is a 30% glass reinforced, lubricated liquid crystal polymer resin designed for enhanced electroless plating.

Celenese acquired the Zenite product line from DuPont in 2010.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.65 g/ccASTM D 792
Filler Content 30 %
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 140 MPa
@Temperature 23.0 °C
ASTM D 638
Elongation at Break 4.0 %
@Temperature 23.0 °C
ASTM D 638
Flexural Strength 150 MPaASTM D 790
Flexural Modulus 11000 MPa
@Temperature 23.0 °C
ASTM D 790
Izod Impact, Notched 3.45 J/cm
@Temperature 23.0 °C
ASTM D 256
Izod Impact, Unnotched 858 J/m
@Temperature 23.0 °C
ASTM D 4812
 
Electrical PropertiesOriginal ValueComments
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear -4.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
 -4.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
 1.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 260 °C
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 2.00 mm,
Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 23.0 °C
ISO 11359-1/-2
 2.00 µm/m-°C
@Thickness 4.00 mm,
Temperature -40.0 - 260 °C
ISO 11359-1/-2
 3.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 3.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 3.00 µm/m-°C
@Thickness 2.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 4.00 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
CTE, linear, Transverse to Flow 58.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2; 2mm
 60.0 µm/m-°C
@Temperature -40.0 - 23.0 °C
ISO 11359-1/-2; 4mm
 85.0 µm/m-°C
@Temperature -40.0 - 260 °C
ISO 11359-1/-2; 2mm
 88.0 µm/m-°C
@Temperature -40.0 - 260 °C
ISO 11359-1/-2; 4mm
 66.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 69.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 23.0 - 55.0 °C
ISO 11359-1/-2
 88.0 µm/m-°C
@Thickness 2.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 91.0 µm/m-°C
@Thickness 4.00 mm,
Temperature 55.0 - 160 °C
ISO 11359-1/-2
 105 µm/m-°C
@Thickness 2.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
 110 µm/m-°C
@Thickness 4.00 mm,
Temperature 160 - 260 °C
ISO 11359-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 260 °CISO 75-1/-2
UL RTI, Electrical 130 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical with Impact 130 °C
@Thickness 1.50 mm
UL 746B
UL RTI, Mechanical without Impact 130 °C
@Thickness 1.50 mm
UL 746B
Flammability, UL94 V-0
@Thickness 1.50 mm
IEC 60695-11-10
 V-0
@Thickness 1.50 mm
UL94
 
Processing PropertiesOriginal ValueComments
Melt Temperature 335 °COptimum
 330 - 350 °C
Mold Temperature 80.0 °COptimum
 40.0 - 150 °C
Drying Temperature 150 °C
Dry Time 3 hourDehumidified Dryer
Moisture Content <= 0.010 %
 
Descriptive Properties
ColorNatural
Drying RecommendedYes
FillerGlass Reinforced
FormsPellets
GenericLCP
Part Marking Code>LCP-GF30<ISO 11469
Polymer FamilyLCP
Polymer TypeLCP
Processing MethodInjection Molding
Product CategoryElectrical Resins
 Glass Reinforced Resins
Region AvailableAmericas
 Asia/Pacific
 Europe
Resin IdentificationLCP-GF30ISO 1043

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Celanese Zenite® 5145L BK010 LCP
Avient Therma-Tech™ LC-6000 TC Liquid Crystal Polymer (LCP)
Celanese ZENITE 6130L LCP, 30% Glass Reinforced
Celanese Zenite® 6130 BK010 LCP, 30% glass reinforced (Extended Tabular Temperature Data)
Celanese Zenite® 6635 BK010 LCP

PDTA7793 / 89916

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.