MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Cabot LITX® 50 Conductive Additive
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Performance conductive additive for lithium-ion batteries
LITX 50 high performance conductive additive for Li-ion batteries balances the need for conductivity and easy processing. LITX 50 conductive additive is primarily used in positive electrodes in loadings ranging from 1-10%, but it can also be used on negative electrodes. Due to its unique morphology, LITX 50 conductive additive requires less solvent during the preparation of electrode pastes which not only enables processing advantages, but often also leads to improved electrode adhesion. These attributes make it a good choice for various Li-ion battery applications that require balance between performance, quality and cost.
Incorporating LITX 50 conductive additive into electrode paste can:
  • Enable higher solids loadings
  • Reduce amount of solvent and conductive additive required
  • Provide higher packing density
  • Improve performance at low temperatures
Battery Applications:
  • Hybrid electric vehicles
  • Tablets
  • Smartphones
  • Power tools

Information provided by Cabot Corporation

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Surface Area 125 - 145 m²/g125 - 145 m²/gBET nitrogen; ASTM D6556
 
Descriptive Properties
Content<10 ppmIron
 <5 ppmTotal Co, Cr, Cu, Mn, Ni

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PCABOT151 / 315886

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.