MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Eastman Velate™ 368 Coalescent
Categories: Fluid

Material Notes: CAS No. 5444-75-7

Velate™ 368 is low odor and low viscosity coalescent. By virtue of having lower odor than most coalescents, paints formulated with Velate™ 368 have minimal or no odor in freshly painted rooms. The principal use of Velate™ 368 is as a coalescent for trade sales latex paints.

Application/Uses:

  • Coatings - Architectural
Key Attributes:
  • Good coalescing efficiency
  • Low odor
  • LVP-VOC
  • Non-HAP
  • Non-SARA
  • Non-yellowing
  • REACH compliant
  • Readily biodegradable

Information provided by Eastman

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.962 g/cc0.0348 lb/in³
Viscosity 20 cP
@Temperature 0.000 °C
20 cP
@Temperature 32.0 °F
 
Thermal PropertiesMetricEnglishComments
CTE, linear 72.0 µm/m-°C40.0 µin/in-°F
Boiling Point 297 °C567 °F@ 760 mm Hg
Pour Point <= -57.0 °C<= -70.6 °F
Flash Point 162 °C324 °FOpen Cup
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.4891.489
 
Descriptive Properties
Color<40 Pt-Co

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PEATM5630 / 222824

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.