MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Pressure Seal 8757 Fluorinated Hydrocarbon
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Compound 8757 is a 75 durometer green colored fluorinated hydrocarbon elastomer, it is formulated with Viton GFLT which imparts excellent chemical resistance. This has improved low temperature flexibility when compared to comparable fluid resistance elastomers.

Information provided by Pressure Seals Inc.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 2.06 g/cc2.06 g/cc
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 7474
 64
@Treatment Temp. 200 °C,
Time 252000 sec
64
@Treatment Temp. 392 °F,
Time 70.0 hour
Stauffer Blend 7700
 67
@Treatment Temp. 100 °C,
Time 252000 sec
67
@Treatment Temp. 212 °F,
Time 70.0 hour
Distilled water aged
 70
@Treatment Temp. 200 °C,
Time 252000 sec
70
@Treatment Temp. 392 °F,
Time 70.0 hour
Service Fluid 101
 72
@Treatment Temp. 150 °C,
Time 252000 sec
72
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 73
@Treatment Temp. 23.0 °C,
Time 252000 sec
73
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 73
@Treatment Temp. 150 °C,
Time 252000 sec
73
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
 77
@Treatment Temp. 250 °C,
Time 252000 sec
77
@Treatment Temp. 482 °F,
Time 70.0 hour
Heat Aged
 78
@Treatment Temp. 275 °C,
Time 252000 sec
78
@Treatment Temp. 527 °F,
Time 70.0 hour
Heat Aged
Tensile Strength 6.65 MPa965 psi
 4.764 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
690.9 psi
@Treatment Temp. 392 °F,
Time 70.0 hour
Stauffer Blend 7700
 4.810 MPa
@Treatment Temp. 23.0 °C,
Time 252000 sec
697.7 psi
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 6.301 MPa
@Treatment Temp. 200 °C,
Time 252000 sec
913.9 psi
@Treatment Temp. 392 °F,
Time 70.0 hour
Service Fluid 101
 6.886 MPa
@Treatment Temp. 150 °C,
Time 252000 sec
998.8 psi
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 7.0926 MPa
@Treatment Temp. 150 °C,
Time 252000 sec
1028.7 psi
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
 7.2098 MPa
@Treatment Temp. 275 °C,
Time 252000 sec
1045.7 psi
@Treatment Temp. 527 °F,
Time 70.0 hour
Heat Aged
 7.8131 MPa
@Treatment Temp. 250 °C,
Time 252000 sec
1133.2 psi
@Treatment Temp. 482 °F,
Time 70.0 hour
Heat Aged
Elongation, Ultimate 256 %256 %
 160 %
@Treatment Temp. 250 °C,
Time 252000 sec
160 %
@Treatment Temp. 482 °F,
Time 70.0 hour
Heat Aged
 160 %
@Treatment Temp. 275 °C,
Time 252000 sec
160 %
@Treatment Temp. 527 °F,
Time 70.0 hour
Heat Aged
 203 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
203 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
ASTM Reference Fuel C
 219.1 %
@Treatment Temp. 200 °C,
Time 252000 sec
219.1 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Stauffer Blend 7700
 219.9 %
@Treatment Temp. 150 °C,
Time 252000 sec
219.9 %
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #3
 226.1 %
@Treatment Temp. 150 °C,
Time 252000 sec
226.1 %
@Treatment Temp. 302 °F,
Time 70.0 hour
ASTM Oil #1
 235 %
@Treatment Temp. 200 °C,
Time 252000 sec
235 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Service Fluid 101
100% Modulus 3.28 MPa475 psi
Tear Strength 14.0 kN/m80.0 pliDie C
 21.2 kN/m121 pliDie B
Compression Set  16.1 %
@Treatment Temp. 23.0 °C,
Time 79200 sec
16.1 %
@Treatment Temp. 73.4 °F,
Time 22.0 hour
Plied
 18.7 %
@Treatment Temp. 175 °C,
Time 79200 sec
18.7 %
@Treatment Temp. 347 °F,
Time 22.0 hour
Plied
 24.9 %
@Treatment Temp. 200 °C,
Time 79200 sec
24.9 %
@Treatment Temp. 392 °F,
Time 22.0 hour
Plied
 
Thermal PropertiesMetricEnglishComments
Brittleness Temperature -31.1 °C-24.0 °F
Shrinkage  -0.100 %
@Treatment Temp. 150 °C,
Time 252000 sec
-0.100 %
@Treatment Temp. 302 °F,
Time 70.0 hour
Volume, ASTM Oil #1
 1.6 %
@Treatment Temp. 150 °C,
Time 252000 sec
1.6 %
@Treatment Temp. 302 °F,
Time 70.0 hour
Volume, ASTM Oil #3
 4.4 %
@Treatment Temp. 23.0 °C,
Time 252000 sec
4.4 %
@Treatment Temp. 73.4 °F,
Time 70.0 hour
Volume, ASTM Reference Fuel C
 6.8 %
@Treatment Temp. 100 °C,
Time 252000 sec
6.8 %
@Treatment Temp. 212 °F,
Time 70.0 hour
Volume, Distilled water aged
 9.0 %
@Treatment Temp. 200 °C,
Time 252000 sec
9.0 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Volume, Service Fluid 100
 16.4 %
@Treatment Temp. 200 °C,
Time 252000 sec
16.4 %
@Treatment Temp. 392 °F,
Time 70.0 hour
Volume, Stauffer Blend 7700
 
Descriptive Properties
ColorGreen

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PPRESL105 / 318315

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.