MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Go Yen Chemical GY-AL-33 High Performance Oil Powder Matting Agent
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: Advantages:
  • Reduce gloss
  • Soft effect
  • Anti-settling
  • Black stain resistant soles
  • Anti-scratch shifting
  • Anti-sticking
Applications:
  • A variety of matting and plain products
  • Water-based and latex paint systems, coatings
  • Solvent-free and water-based PU
  • UV-curable acrylic systems
  • Film coating
  • Flooring, furniture, paint protection
  • Textile adhesive resin
  • Industrial and decorative coatings, inks

Information provided by Go Yen Chemical

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Brightness 95.0 %95.0 %Whiteness
Oil Absorption 320 %320 %
pH 6.0 - 7.06.0 - 7.0
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) <= 9.0 %
@Temperature 1000 °C,
Time 7200 sec
<= 9.0 %
@Temperature 1830 °F,
Time 2.00 hour
 
Descriptive Properties
AppearanceFine Powder
ColorWhite
Loss on drying<5%2 hr @105°C
Porosity1.8-2.0 ml/g

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PGOYEN457 / 266765

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.