MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Lucite International Diakon® Frost 952 80 Acrylic Polymer
Categories: Polymer; Thermoplastic; Acrylic (PMMA); Acrylic, General Purpose, Molded

Material Notes:

Information provided by Lucite International

Key Words: PMMA; Polymethyl Methacrylate; Polymethylmethacrylate
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.19 g/cc0.0430 lb/in³ISO 1183
Water Absorption 0.30 %0.30 %ISO 62
Melt Flow 1.5 g/10 min1.5 g/10 minISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Rockwell M 9090ISO 2039-2
Ball Indentation Hardness 170 MPa24700 psiISO 2039-1 (H 961-30)
Tensile Strength 72.0 MPa10400 psiISO 527
Elongation at Break 6.4 %6.4 %ISO 527
Flexural Strength 120 MPa17400 psiISO 178
Flexural Modulus 3.20 GPa464 ksiISO 178
Izod Impact, Notched (ISO) 1.60 kJ/m²0.761 ft-lb/in²ISO 180/1A
Charpy Impact Unnotched 2.20 J/cm²10.5 ft-lb/in²ISO 179/1eU
Charpy Impact, Notched 0.200 J/cm²0.952 ft-lb/in²ISO 179/1eA
 
Thermal PropertiesMetricEnglishComments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C210 °FISO 75B
Deflection Temperature at 1.8 MPa (264 psi) 95.0 °C203 °FISO 75A
Vicat Softening Point 101 °C214 °FISO 306B
 108 °C226 °FISO 306A
Flammability, UL94 HBHB
Glow Wire Test 650 °C1200 °FIEC 695-2-1
 
Optical PropertiesMetricEnglishComments
Haze 88.8 %88.8 %ASTM D1003
Transmission, Visible 87.3 %87.3 %ASTM D1003

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
CENTROPLAST CENTRODAL C Polyoxymethylene Copolymer
Lucite International Diakon® ST25G6 Toughened Acrylic Polymer
Lucite International Diakon® ST15G6 Toughened Acrylic Polymer
Lucite International Diakon® Rapide CLG 356B Enhanced Molding Acrylic Polymer
Lucite International Diakon® LG156 Acrylic Bead Polymer, High Transparency

PLUCIT916 / 147550

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.