MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil Mobil 1 20W-50 Motorcycle Oil V-Twin 4-Cycle
Categories: Fluid; Lubricant

Material Notes: Mobil 1 Motorcycle Oils are formulated with 100 percent synthetic fluids. The unique, synthetic structure of the Mobil 1 Motorcycle formulations enable them to offer advantages well beyond conventional motorcycle oils of similar viscosities. For example, conventional base oils change viscosity as the temperature changes, much more so than synthetic fluids. This characteristic forces manufacturers of conventional, multigrade motorcycle oils to use additive thickeners which will help the oil maintain its viscosity as temperature increases. These thickeners can shear down and lose their thickening capacity in an operating engine or transmission. Synthetic fluids do not require much thickener to achieve a multigrade viscosity rating and, in some cases, do not require any thickener. Hence, synthetic formulations will provide a more shear stable, protective oil film for engine bearings, piston rings, transmission gears, etc. than will a conventional oil of a similar viscosity grade. All three Mobil 1 Motorcycle formulations offer excellent flow characteristics at low temperatures to reduce engine wear at start-up, and outstanding resistance to oxidation and/or volatilization at high temperatures, both of which degrade the oil. Further, the Mobil 1 Motorcycle Oils provide outstanding protection against engine wear under high-temperature, high engine speed conditions. Each of the Mobil 1 Motorcycle product formulations have been optimized to meet the unique performance characteristics demanded by motorcycle engines and thus, provide an even higher level of performance and protection for motorcycle engines than the Mobil 1 Automotive engine oils.

Mobil 1 Motorcycle Oils are full synthetic, high-performance engine oils formulated specifically to meet the demanding needs of motorcycle engines. Mobil 1 MX4T 10W-40 is designed primarily for on-road, high-performance, 4-cycle sport bikes, however, it may be used in other types of on and off-road 4-cycle motorcycles. Mobil 1 V-Twin 20W-50 is formulated to offer outstanding protection in 4-cycle, V-Twin type engines, particularly those which are air cooled and tend to run hotter than other types of engines. Mobil 1 MX2T is a full-synthetic 2-cycle engine oil which provides exceptional lubricity to help prevent piston scuffing, and excellent protection against exhaust port clogging, in high-performance, 2-cycle motorcycle engines. Mobil 1 MX4T 10W-40 and Mobil 1 V-Twin 20W-50 are recommended for 4-cycle, motorcycles which specify the use of a 10W-40 or a 20W-50 engine oil, respectively. These products will provide excellent performance in motorcycle engines that are designed with a common engine/transmission lubrication system or where the engine lubrication system is separate from the transmission system. In the case of the latter, follow the manufacturers recommendation for the type of fluid to be used in the transmission. Mobil 1 MX4T 10W-40 and Mobil 1 V-Twin 20W-50 engine oils are also designed to provide the proper frictional characteristics necessary for wet-clutch engine/transmission systems. Mobil 1 MX4T 10W-40 and Mobil 1 V-Twin 20W-50 exceed the requirements of API Service Categories SH, SG/CF, CD and have been fully tested, both on laboratory dynamometers and in the field, to provide optimum horsepower and acceleration. Mobil 1 MX2T is recommended for 2-cycle motorcycle engines which specify the use of a pre-mix, 2-cycle engine oil. The manufacturers recommendation for fuel oil ratio should be followed when mixing Mobil 1 MX2T with the fuel. This product is race proven around the world and will provide outstanding lubricity and thermal stability under extreme high-temperature, high-engine speed operating conditions in any 2-cycle, motorcycle engine. Further, Mobil 1 MX2T will help minimize spark plug fouling and exhaust smoke. Mobil 1 MX2T exceeds the API TC, JASO FC and proposed ISO-L-EGD, 2-cycle engine oil performance levels.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.878 g/cc
@Temperature 15.0 °C
API Gravity 29.4 °
Viscosity 2930 cP
@Temperature -10.0 °C
Cold Cranking
 8500 cP
@Temperature -20.0 °C
Pumping
Viscosity Measurement 150Index
Kinematic Viscosity at 40°C (104°F) 130 cSt
Kinematic Viscosity at 100°C (212°F) 17.7 cSt
 
Thermal PropertiesOriginal ValueComments
Pour Point -51.0 °C
Flash Point 270 °CASTM D92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WEXXON065 / 75490

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.