MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Solder Replacement
RoHS Compliant Adhesives for Solder Replacement
Master Bond offers RoHS compliant, electrically conductive systems to replace lead soldering. These epoxy and silicone adhesives offer low volume resistivity, low outgassing and high temperature resistance.

(Viewing data as-entered. Click here to return)
Lucas-Milhaupt HI-TEMP® 932 Nickel-Phosphorus Brazing Alloy Powder (AWS BNi-6)
Categories: Metal; Nonferrous Metal; Solder/Braze Alloy

Material Notes: Hi-Temp 932 is a low melting nickel-phosphorus brazing alloy powder used in high strength and oxidation applications. Typically, this alloy is used for joining super alloys, stainless steels, and alloys requiring good joint strength at high temperatures while maintaining good corrosion and oxidation resistant characteristics. Hi-Temp 932 exhibits low base metal penetration and is ideal for joining thin metal sections.

Available forms: Powder and paste.

Information provided by Lucas-Milhaupt.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 6.23 g/cc
Density 0.225 lb/in³
 
Thermal PropertiesOriginal ValueComments
Melting Point 1610 °F
Solidus 1610 °F
Liquidus 1610 °F
 
Processing PropertiesOriginal ValueComments
Processing Temperature 1700 - 2000 °FBrazing Range
 
Component Elements PropertiesOriginal ValueComments
Aluminum, Al <= 0.050 %
Carbon, C <= 0.060 %
Cobalt, Co <= 0.10 %
Other, total <= 0.50 %
Phosphorus, P 10 - 12 %
Selenium, Se <= 0.0050 %
Sulfur, S <= 0.020 %
Titanium, Ti <= 0.050 %
Zirconium, Zr <= 0.050 %
 
Descriptive Properties
ColorIron Gray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

NLUCM9871 / 254802

solder replacement adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.