MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

Teknor Apex Sarlink® TPV X6145N Thermoplastic Vulcanizate
Categories: Polymer; Thermoplastic; Elastomer, TPE; Thermoplastic Vulcanizate Elastomer (TPV)

Material Notes: Notes: Sarlink TPV X6100 series are engineered materials designed for consumer, automotive, and industrial applications requiring superior Colorability and elastic performance. This product is a medium hardness, low density, multi-purpose thermoplastic vulcanizate that does not require pre-drying and can be processed by injection molding.

Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North America

Features: Chemical Resistant; Good Adhesion; Good Colorability; Good Flexibility; Good Flow; Good Processability; Medium Hardness; Low Density; Low Specific Gravity; Resilient

Uses: Automotive Applications; Consumer Applications; Industrial Applications; Rubber Replacement; Soft Touch Applications

RoHS Compliance: RoHS Compliant

Form: Pellets

Processing Method: Injection Molding

Information provided by Teknor Apex

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 g/cc0.0322 lb/in³ISO 1183
Viscosity 225 cP
@Shear Rate 206 1/s,
Temperature 200 °C
225 cP
@Shear Rate 206 1/s,
Temperature 392 °F
Shear, Capillary; ASTM D3835
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A  42
@Time 5.00 sec
42
@Time 0.00139 hour
Extruded; ISO 868
 46
@Time 5.00 sec
46
@Time 0.00139 hour
Injection Molded; ISO 868
Tensile Strength at Break 3.10 MPa450 psiFlow; ISO 37
 3.70 MPa537 psiAcross Flow; ISO 37
Tensile Stress at Strain  1.10 MPa
@Strain 100 %
160 psi
@Strain 100 %
Across Flow; ISO 37
 1.60 MPa
@Strain 100 %
232 psi
@Strain 100 %
Flow; ISO 37
Elongation at Break 400 %400 %Flow; ISO 37
 610 %610 %Across Flow; ISO 37
Tear Strength 15.8 kN/m90.0 pliMethod Ba, Angle (Unnicked); ISO 34-1
Compression Set  24 %
@Temperature 22.8 °C,
Time 79200 sec
24 %
@Temperature 73.0 °F,
Time 22.0 hour
ISO 815
 33 %
@Temperature 70.0 °C,
Time 79200 sec
33 %
@Temperature 158 °F,
Time 22.0 hour
ISO 815
 49 %
@Temperature 125 °C,
Time 252000 sec
49 %
@Temperature 257 °F,
Time 70.0 hour
ISO 815
 
Processing PropertiesMetricEnglishComments
Processing Temperature 182 - 227 °C360 - 440 °F
Rear Barrel Temperature 138 - 160 °C280 - 320 °F
Middle Barrel Temperature 166 - 193 °C330 - 380 °F
Front Barrel Temperature 177 - 227 °C350 - 440 °F
Nozzle Temperature 182 - 227 °C360 - 440 °F
Mold Temperature 15.6 - 54.4 °C60.0 - 130 °F
Back Pressure 0.345 - 1.03 MPa50.0 - 150 psi
Screw Speed 25 - 75 rpm25 - 75 rpm
 
Descriptive Properties
AppearanceNatural Color
 Opaque

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
E-Polymers EFLEX® V2045 SEBS/TPV
Chengdu Polyster 4502 High Performance Grade TPV
Barlog Plastics KEBAFLEX E 50.1 TPE-V, Shore A50
Barlog Plastics KEBAFLEX E 45.1 TPE-V, Shore A45
Barlog Plastics KEBAFLEX E 40.1 TPE-V, Shore A40

PTEKNQ1214 / 237705

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.