MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Trelleborg Offshore Vikotherm™ 73585 Insulative Elastomer
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure resistance, mechanical properties and temperatures.

Vikotherm™ systems provide good adhesion between systems and substrates such as Duplex, Super Duplex, Carbon Steel, and Titanium. The product is applied in three layers, the innermost layer provides corrosion protection, the central layer ensures thermal insulation and the outer layer acts as a protective cap, giving protection against impact, abrasion and seawater ingress.

Both the inner and outer layers are made from a soft rubber with good flexibilities and the central layer is of hard rubber in order that thermal conductivity remains low even in deeper water. All of the layers are chemically bonded together and the inner layer is bonded to the steel surface.

This grade is part for the inner layer.

All information provided by Trelleborg Offshore

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.890 - 1.11 g/cc0.0322 - 0.0401 lb/in³
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 65 - 7565 - 75
Tensile Strength, Yield >= 11.0 MPa>= 1600 psi
Elongation at Break >= 5.0 %>= 5.0 %
Tear Strength >= 45.0 kN/m>= 257 pli
 
Thermal PropertiesMetricEnglishComments
Thermal Conductivity 0.130 W/m-K0.902 BTU-in/hr-ft²-°F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PTRELL175 / 83933

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.