MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Specialty Compounds RTP Company

Reynolds Econ® 80 Urethane Mold making Rubber
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: Econ™ 80 is an economical Shore 80A urethane rubber suitable for a variety of mold making and industrial applications. It is a lower cost, faster cure alternative to our popular PMC™-780. Physical properties are lower vs. PMC™-780. This is a no odor system that features a 1A:1B mix ratio and a low viscosity for easy mixing and pouring. Working time is about 13 minutes at room temperature, handling time is 6 hours and rubber cures overnight. Econ™ 80 is translucent and easily colored with SO-Strong™ or Ignite™ colorants. Econ™ 80 is used to make short run molds for casting concrete and resins, concrete stamping pads, rubber mechanical parts, coating fabrics, pour-in-place gaskets for industrial equipment and burial vaults. Important; To minimize air bubbles in cured rubber, vacuum degassing is recommended.

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 1.06 g/cc1.06 g/ccASTM D-1475
Linear Mold Shrinkage 0.0014 cm/cm0.0014 in/in
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 8080ASTM D-2240
Tensile Strength 6.58 MPa955 psiASTM D-412
Elongation at Break 127 %127 %ASTM D-412
100% Modulus 4.62 MPa670 psiASTM D-412
Tear Strength 13.5 kN/m77.0 pliDie C; ASTM D-624
 
Processing PropertiesMetricEnglishComments
Cure Time 1440 min24.0 hour
Pot Life 13.0 min13.0 minASTM D-2471
 
Descriptive Properties
ColorTranslucent
Mix Ratio100A:90Bby weight
 1A:1Bby volume
Specific Volume26.2[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PREYN090 / 296791

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.