System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Huntsman IROGRAN® A 85 P 4441 FCM Ether-Based TPU-For Food Contact
Categories:
Polymer
;
Thermoplastic
;
Elastomer, TPE
;
Polyurethane TPE
;
Polyurethane, TP
;
Thermoplastic Polyurethane, Elastomer, Ether Grade
Material Notes:
Extrusion grade; High microbial resistance, matte surface
Information provided by Huntsman
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Melt Flow
65
g/10 min
65 cm
3
/10 min; Melt Volume Rate
Mechanical Properties
Original Value
Comments
Hardness, Shore A
87
Hardness, Shore D
38
Tensile Strength at Break
40.0
MPa
Elongation at Break
650 %
Tear Strength
60.0
kN/m
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Huntsman IROGRAN® A 85 P 4394 FCM Ether-Based TPU-For Food Contact
Clariant Renol PURSP0002 Polyurethane Elastomer, Ether Based
Covestro Platilon® 4201 AU Polyurethane (Ether) Film
Dow Pellethane® 2351-85AE Polyurethane Elastomer, Ether Based
NEU NEUSoft™ 455-50A Ester/ether TPU / SBC blend
PHU9942 / 150402
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
info@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.