MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Chemically Resistant adhesives

Okulen® OKUSLIDE® PVDF
Categories: Polymer; Thermoplastic; Polyethylene (PE); High Density (HDPE); UHMW PE (Ultra High Molecular Weight PE)

Material Notes: OKUSLIDE® Premium Blue FN5893 is an UHMW PE polymer. By adding of special additives it possesses a low coefficient of friction. The improve low coefficient of friction (non-stick surface) makes this material ideal for lining applications were sticking or caking creates a build up of material. In such application were there is a material flow problem, time and money is at a loss. Our UHMW PE liner will help you solve these problems.

Properties: Excellent sliding properties; Low coefficient of friction; Good notched impact strength; Very good wear resistance; Probably no sticking or caking of bulk materials; UV stabilized; EU & FDA conform for food contact

Color: blue FN5893/similar RAL 5019

Range of applications: Truck liners for tippers; Conveyor industry (earth moving equipment)

Information provided by Okulen

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.930 g/cc0.0336 lb/in³DIN EN ISO 11831-1
Water Absorption <= 0.010 %<= 0.010 %DIN EN ISO 62
Molecular Weight 3.00e+6 - 5.00e+6 g/mol3.00e+6 - 5.00e+6 g/mol
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 62
@Time 3.00 sec
62
@Time 0.000833 hour
6 mm plate; DIN EN ISO 868
Tensile Strength, Yield >= 17.0 MPa>= 2470 psi1B- 50 mm/min; DIN EN ISO 527-2
Elongation at Break >= 250 %>= 250 %1B- 50 mm/min; DIN EN ISO 527-2
Tensile Modulus >= 0.650 GPa>= 94.3 ksi1B- 1 mm/min; DIN EN ISO 527-2
Izod Impact, Notched (ISO) >= 150 kJ/m²>= 71.4 ft-lb/in²DIN EN ISO 21304-2
Coefficient of Friction, Dynamic 0.0900.090ASTM D1894
Coefficient of Friction, Static 0.150.15ASTM D1894
Abrasion 100100Sand-Slurry; DIN EN ISO 15527
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity >= 1.00e+14 ohm-cm>= 1.00e+14 ohm-cmDIN EN 62631-3-1
Surface Resistance >= 1.00e+13 ohm>= 1.00e+13 ohmDIN EN 62631-3-2
 
Thermal PropertiesMetricEnglishComments
CTE, linear, Parallel to Flow 15.0 - 20.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
8.33 - 11.1 µin/in-°F
@Temperature 73.4 - 176 °F
ISO 11359
Thermal Conductivity 0.410 W/m-K2.85 BTU-in/hr-ft²-°F
Melting Point 135 - 137 °C275 - 279 °FDIN EN ISO 11357-1
Flammability, UL94 HBHB
 
Descriptive Properties
Operation Temperature80°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

POKUL1053 / 307330

Chemically Resistant adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.