MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
CHT ALPA-SIL 36202 Silicone Molding Rubber
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Description: This is a pourable 2-part addition cure silicone elastomer system. After mixing parts ‘A’ and ‘B’ in the correct proportions, the system will cure at ambient temperatures within 24 hours, but the rate of cure can be accelerated by heat. The cured rubber exhibits excellent physical and electrical properties.

Key Features

  • Crosslinks at temperatures as of 23 °C/77°F
  • Easy mixing of the components
  • Simple processing
  • Very good alkali stability and therefore excellently suited for concrete moulds
Application: Moulds for concrete

Information provided by CHT Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Brookfield Viscosity 35000 cPA
 35000 cPB
 35000 cPMixed
Linear Mold Shrinkage 0.0010 cm/cm
Storage Temperature <= 30.0 °C
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 36DIN 53 505
Tensile Strength 870 psiISO 37
Elongation at Break 330 %ISO 37
Tear Strength 92.0 pliBS ISO 34-1
 
Processing PropertiesOriginal ValueComments
Cure Time 10.0 - 12.0 hourTack Free Time / Skin Formation
 14.0 hourDe-mould Time / Full Cure
Pot Life 60.0 - 90.0 min
Shelf Life 12.0 Month
 
Descriptive Properties
AppearanceWhite
ColorWhiteA
 WhiteCured Product
Cure typeAddition
Mix Ratio1:1By Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHTSIL091 / 314574

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.