Process Stability TOTAL Petrochemicals Polypropylene 3866 features excellent processability and gas fade resistance. FDA. 3866 complies with all applicable FDA regulations for food contact applications Recommended Applications. 3866 is recommended for spunbond nonwoven fabric high speed melt spinning applications, multifilament yarns, and extrusion coating. Information provided by Total Petrochemicals. |