Base Polymer: Polycarbonate Filler/Additive System: special filler Special Features: Light scattering, high light transmission, good flow, UV stabilized, injection molding grade Market Segment: Automotive, Lighting Application Area: Lighting, light transparent components Typical Application: Lamp covers, display elements, operating elements Information provided by Albis Plastics |