MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Reynolds TASK® 9 High performance urethane casting resin
Categories: Polymer; Thermoset; Polyurethane, TS; Thermoset Polyurethane, Elastomer, Unreinforced

Material Notes: Product Overview: TASK™ 9 Colormatch is a high performance urethane casting resin that features very high compressive strength and tensile strength. TASK™ 9 is clear amber, which makes this plastic very easy to color using SO-Strong™ or IGNITE™ colorants. With a mix ratio of 1A:1B by volume, TASK™ 9 is easy to use and a low mixed viscosity (300 cps) ensures minimal bubble entrapment. Pot life is 7 minutes and cure time is about 60 minutes (depending on mass). TASK™ 9 is ideal for making impact resistant tooling, color accurate prototypes / models as well as durable reproductions. This resin is designed for casting in thicknesses up to ½” (1.27 cm).

Information provided by Reynolds Advanced Materials

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.14 g/ccASTM D-1475
Viscosity 300 cPMixed; ASTM D-2393
Linear Mold Shrinkage 0.0090 in/inASTM D-2566
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 85ASTM D-2240
Tensile Strength, Ultimate 7800 psiASTM D-638
Elongation at Break 6.0 %ASTM D-638
Tensile Modulus 370000 psiASTM D-638
Flexural Strength 11850 psiASTM D-790
Flexural Modulus 350000 psiASTM D-790
Compressive Strength 11000 psiASTM D-695
Compressive Modulus 98000 psiASTM D-695
 
Thermal PropertiesOriginal ValueComments
Heat Distortion Temperature 55.0 °CASTM D-648
 
Processing PropertiesOriginal ValueComments
Cure Time 60.0 minHandling Time
Pot Life 7.00 minASTM D-2471
 
Descriptive Properties
ColorClear Amber
Mix Ratio115A:100Bby weight
 1A:1Bby volume
Specific Volume24.3[cu. in./lb.]

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PREYN036 / 296737

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.