MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Matrix 999225 Composite Syntactic Foam
Categories: Other Engineering Material; Composite Core Material

Material Notes: Composite syntactic materials made from a combination of microspheres, liquid epoxy resins (matrix material) and re-enforcing fillers.

Information provided by Matrix Composites & Engineering

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.327 g/ccASTM D1622
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 3.70 MPaASTM D1623
Tensile Modulus 853 MPaASTM D1623
Compressive Strength 11.0 MPaASTM D1621
Compressive Modulus 419 MPaASTM D1621
Shear Strength 3.10 MPaASTM C393
 
Descriptive Properties
Buoyancy loss 20 years at depth<2%Matrix Proprietary std.
Hydrostatic Crush Strength15 MPaMatrix Proprietary std.
Hydrostatic Modulus620 MPaMatrix Proprietary std.
Service Depth500 m

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Carbon-Core Carbon Balsa Wood
Evonik Rohacell® 110 A Aircraft Grade Polymethacrylimide (PMI) Foam
3M Balsa Panels
CoreLite BALSASUD® Core UL Ultra Lite Balsa Core Material
Engineered Syntactic Systems MZ-32 Deep Water Syntactic Foam

PMATRIX01 / 185386

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.