COPYLENE® CR020N is a random copolymer formulated with advanced nucleator technology and is specially designed to excel in extrusion blowmolding processes. EBM bottles will have exceptional gloss and low haze. Applications: Extrusion Blowmolding Processes Information provided by Phillips 66. |
Exceptional gloss and low haze |