MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Rogers Arlon 31580R015 0.015" (0.381 mm) Uncured Unsupported Silicone Rubber on an HDPE Carrier  (discontinued **)
Categories: Polymer; Thermoset; Silicone; Silicone Rubber

Material Notes: Design/Construction:
Side 1: Uncured Unsupported Silicone Rubber on a HDPE Carrier

Appearance: Red silicone gum on polymer liner

This data represents typical values for the production material. The data should not be used to write, or in place of, material specifications

Information provided by Arlon Silicone Technologies Division; now a part of Rogers Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Thickness 76.2 microns3.00 milPolyethylene Interleave
 178 microns7.00 milHDPE Carrier
 343 - 419 microns13.5 - 16.5 milOverall
 343 - 419 microns13.5 - 16.5 milSide 1
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 40 - 5040 - 50Compound Property
Tensile Strength >= 5.52 MPa>= 800 psiCompound Property
Elongation at Break 500 %500 %Compound Property
Peel Strength 1.05 kN/m6.00 pliBond Strength
 
Electrical PropertiesMetricEnglishComments
Dielectric Strength >= 15.7 kV/mm>= 400 kV/in
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 200 °C392 °Frated per UL card E54153
Minimum Service Temperature, Air -56.7 °C-70.0 °F
Flammability, UL94 HBHB
 
Processing PropertiesMetricEnglishComments
Cure Time 120 min
@Temperature 204 °C
2.00 hour
@Temperature 400 °F
Recommended Postcure Cycle
 15.0 min
@Pressure 0.345 MPa,
Temperature 177 °C
0.250 hour
@Pressure 50.0 psi,
Temperature 350 °F
Recommended Cure Cycle
Shelf Life 6.00 Month
@Temperature 23.9 °C
6.00 Month
@Temperature 75.0 °F
From date of manufacture
 
Descriptive Properties
ColorRed
Total Product Weight (oz/yd2)14.2 - 17.2

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Eastman Eastar GN101 PETG Copolyester
Eastman Eastar K3000 PETG Copolyester
Bakelite® PF 1142 Phenolic Formaldehyde Resin, High Mechanical Strength
Excelite Plastic Polycarbonate solid sheet
GEHR Plastics PA 6 G Nylon 6, Cast, Conditioned

PARL163 / 125349

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.