MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Ensinger PEI

(Viewing data as-entered. Click here to return)
Phillips 66 Open Gear Lube Grade 585 NC
Categories: Fluid; Lubricant

Material Notes: Phillips 66® Open Gear Lube is a viscous, tacky, petroleum resin-based gear lubricant cut back with a volatile, non-chlorinated solvent for ease of application. It is recommended primarily for the lubrication and cushioning of open and semi-enclosed gears on mining shovels, draglines and excavation equipment used in underground and surface mines and in rock quarries. It also may be used for the lubrication of some cable-actuated equipment. Open Gear Lube is specially formulated to provide high load-carrying capacity to protect heavily loaded gears from scoring and galling. It forms a heavy, tenacious film (after solvent evaporation) that adheres well to metal surfaces and will not harden or flake off at low temperatures. This film provides good resistance to water washout and protects gears against rust and corrosion. Open Gear Lube is available in three grades for use over a wide range of operating temperatures.

Applications:

  • Open and semi-enclosed gears found on mining shovels, draglines and excavation equipment
  • Guides and sliding surfaces with large clearances, where asphaltic-type lubricants are specified
  • Cables on draglines, clamshells, hoists and other cable-operated equipment where cable clamp safety devices are not used
Open Gear Lube meets the requirements of the following industry specification:
  • ANSI/AGMA Standard 9005-E02)
Features/Benefits:
  • Excellent adhesion to metal surfaces
  • Forms a heavy, tenacious film to lubricate and cushion gear teeth
  • Good extreme-pressure properties for protection under heavy or shock loads
  • Good resistance to water washout
  • Protects against rust and corrosion
  • Will not flake off at low temperatures
  • Does not contain any chlorine, lead or carcinogens
  • Easy application, by spraying, brushing or dripping
  • Suitable for use with automatic lubrication equipment

Information provided by Phillips 66 Lubricants.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.978 g/cc
Density 8.14 lb/gal
Saybolt Viscosity at 210°F 2600 SUS
Kinematic Viscosity at 40°C (104°F) 540 cSt
 
Mechanical PropertiesOriginal ValueComments
Four Ball Extreme Pressure, Load Wear Index 65ASTM D2596
Four Ball Extreme Pressure, Weld Load 400 kgASTM D2596
Four Ball Wear 0.500 mmScar Diameter; ASTM D4172
Timken Test 45.0 lbASTM D2782
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 10.0 °C
Minimum Service Temperature, Air -18.0 °C
Flash Point >= 93.0 °CCOC, with solvent
 
Descriptive Properties
ColorBlack
Copper Corrosion4aASTM D130

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

WCON5396 / 198649

Proto3000 – 3D Engineering Solutions

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.