MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Synthos 8000 CPE Resin
Categories: Other Engineering Material; Additive/Filler for Polymer

Material Notes: CPE is one of the most important impact modifiers for the universal plastics market. Compared with other impact modifiers like AIM (Acrylic Impact Modifier), MBS and ABS.

Characteristics: Highest molecular weight, lower chlorine content, higher modulus, excellent mechanical performance, high filler acceptance, good gelation, excellent processability, high gloss and excellent surface for end products

Application: High quality window profile application

Information provided by Sundow Polymers Co., Ltd

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Bulk Density 0.540 g/cc0.0195 lb/in³
Volatiles 0.20 %0.20 %
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore A 6363
Tensile Strength 12.0 MPa1740 psi
Elongation at Break 800 %800 %
 
Thermal PropertiesMetricEnglishComments
Heat of Fusion 1.00 J/g0.430 BTU/lb
 
Component Elements PropertiesMetricEnglishComments
Chlorine, Cl 30 %30 %
 
Descriptive Properties
AppearanceWhite powder
Content8 piece/100gImpurity particles
Sieve residue00.8mm sieve
Thermal stability time12 minat 165°C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PSUNDOW249 / 320280

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.