MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Fibre Glast 1099 Room Temperature Epoxy Surface Coat
Categories: Polymer; Thermoset; Epoxy; Epoxy, Cast, Unreinforced

Material Notes: Safety hardener with fast overnight cure. Low viscosity thins the resin well for best detail reproduction. Can be sanded in 16-18 hours.

#1099 is a white, medium viscosity epoxy surface coat that can be used with several hardeners for a range of cured and handling characteristics. #1099 is a versatile material, and will perform well in a variety of room temperature applications. #1099 produces excellent reproduction of very fine detailed surfaces. it is often chosen for broad, flat tooling surfaces, where it can be applied fast. #1099 has been formulated to provide good bonds to subsequently applied layers of epoxy. This feature provides good intercoat bonds, even if the previous layer of #1099 has cured completely hard. This elimination of surface coat adhesion failures is accomplished with no sacrifice in properties. #1099 is an excellent material for all types of general tooling uses.

Information provided by Fibre Glast Developments Corporation.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 9090ASTM D2240
Tensile Strength at Break 37.9 MPa5500 psiASTM D638
Flexural Strength 40.7 MPa5900 psiASTM D790
Compressive Yield Strength 82.7 MPa12000 psiASTM D695
 
Processing PropertiesMetricEnglishComments
Cure Time 1080 - 1440 min
@Temperature 25.0 °C
18.0 - 24.0 hour
@Temperature 77.0 °F
Pot Life 20 - 25 min20 - 25 min
 
Descriptive Properties
ColorLight Oxide Red
Mix Ratio100:11Resin:Hardener by Weight

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PFIBRE20 / 38291

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.