MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

KLJ Group KANATOL 80 S Plasticizer
Categories: Fluid

Material Notes: Properties: K-80S is low colour and low odour oily liquid, free of foreign materials.

Application: It is used widely in the metal working industry as a lubricant. Commonly used emollient in makeup and skin care products.

Chemical Name: 2-Ethylhexyl Stearate

Molecular Formula: C 26 H52 O2

Molecular Structure: C 17 H25 COOC8 H17

CAS Number: 22047-49-0

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Specific Gravity 0.855 - 0.861 g/cc
@Temperature 27.0 °C
0.855 - 0.861 g/cc
@Temperature 80.6 °F
ASTM D1045-08
Viscosity 16 - 22 cP16 - 22 cPKLJ TM-P-13-97
Molecular Weight 396 g/mol396 g/mol
 
Thermal PropertiesMetricEnglishComments
Flash Point 425 °C797 °F
 
Optical PropertiesMetricEnglishComments
Refractive Index 1.44 - 1.446
@Temperature 27.0 °C
1.44 - 1.446
@Temperature 80.6 °F
ASTM D1045-08
 
Processing PropertiesMetricEnglishComments
Moisture Content <= 0.10 %<= 0.10 %ASTM E203-08
Shelf Life 24.0 Month24.0 Month
 
Descriptive Properties
Acidity as Acid<0.5%ASTM D1045-08
AppearanceWater White Clear Liquid
Color<60Hazen, ASTM D1045-08
Content>99.5%Ester Content, ASTM D1045-08
 >99.5%Plasticizing Ester by GLC, KLJ TM-P-12-98
 140-146 mg KOH/gmEster Value, ASTM D1045-08
 2.5 ppmIodine Value
Volatile Loss<0.2%130°C for 3 hrs, KLJ TM-P-11-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PKLJ246 / 284267

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.