MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Magnesium
Magnesium Elektron - Service & Innovation in Magnesium

Magnesium Elektron SoluMag™ Controlled High Corrosion Magnesium Alloy
Categories: Metal; Nonferrous Metal; Magnesium Alloy

Material Notes: SoluMag is a high strength magnesium alloy that has a high corrosion rate in aqueous chloride environments. This lightweight alloy is available as balls, extruded rods, bars and profiles to produce components that have high strength and ductility in demanding environments as well as a controlled corrosion rate that will effectively dissolve the component in a known time.

Applications:

  • Balls for hydraulic fracturing systems
  • Machined components for downhole completion tools in Oil & Gas applications
  • Time activated sub-sea devices
  • Flooding plugs for IP protection

Information provided by Magnesium Elektron.

Vendors: Magnesium Elektron is the world leader in high strength magnesium alloys in rolled, extruded and cast forms. Phone (303) 589-3189 or visit www.magnesium-elektron.com.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Mechanical PropertiesMetricEnglishComments
Tensile Strength, Ultimate  310 MPa
@Thickness >=76.2 mm
45000 psi
@Thickness >=3.00 in
 315 MPa
@Thickness 25.4 - 76.2 mm
45700 psi
@Thickness 1.00 - 3.00 in
 340 MPa
@Thickness <=25.4 mm
49300 psi
@Thickness <=1.00 in
Tensile Strength, Yield  200 MPa
@Strain 0.2 %,
Thickness >=76.2 mm
29000 psi
@Strain 0.2 %,
Thickness >=3.00 in
 210 MPa
@Strain 0.2 %,
Thickness 25.4 - 76.2 mm
30500 psi
@Strain 0.2 %,
Thickness 1.00 - 3.00 in
 240 MPa
@Strain 0.2 %,
Thickness <=25.4 mm
34800 psi
@Strain 0.2 %,
Thickness <=1.00 in
Elongation at Break  19 %
@Thickness 25.4 - 76.2 mm
19 %
@Thickness 1.00 - 3.00 in
 19 %
@Thickness >=76.2 mm
19 %
@Thickness >=3.00 in
 20 %
@Thickness <=25.4 mm
20 %
@Thickness <=1.00 in
 
Descriptive Properties
Corrosion rate1300-1500 mg/cm2/day200°F aqueous KCl
 200-400 mg/cm2/day100°F aqueous KCl

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Magnesium Elektron Elektron® ZK60A Magnesium Alloy, UNS M16600
SAE SiC/AZ91 Magnesium Matrix Composite, as cast
Magnesium EA55RS-T4, Extruded
Magnesium EA65RS-T4, Extruded
SAE AZ91 Magnesium Matrix Composite, as cast

NMAGEL914 / 186929

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.