MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

Borealis Borseal™ RE939CF Polypropylene Copolymer  (discontinued **)
Categories: Polymer; Thermoplastic; Polypropylene (PP); Polypropylene Copolymer

Material Notes: Borseal™ RE939CF is a random copolymer. This grade is suitable for the manufacturing of unoriented films on chill roll processes. Applications: Borseal™ RE939CF is designed for: Food packaging, lamination films, and stationary films.

Information provided by Borealis AG

Key Words: PP
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 0.905 g/cc0.0327 lb/in³ISO 1183
Melt Flow 12 g/10 min
@Load 2.16 kg,
Temperature 230 °C
12 g/10 min
@Load 4.76 lb,
Temperature 446 °F
ISO 1133
Slip Level 2000 ppm2000 ppmEAA; Borealis Method
 
Mechanical PropertiesMetricEnglishComments
Tensile Modulus 0.300 GPa43.5 ksiMD/TD; ISO 527-3
Flexural Modulus 0.550 GPa79.8 ksiISO 178
Dart Drop, Total Energy 30.0 J22.1 ft-lb900N; ISO 7765-2
Coefficient of Friction >= 0.20>= 0.20ISO 8295
Film Tensile Strength at Break, MD 25.0 MPa3630 psiISO 527-3
Film Tensile Strength at Break, TD 25.0 MPa3630 psiISO 527-3
 
Thermal PropertiesMetricEnglishComments
Melting Point 137 °C279 °FDSC; ISO 3146
Deflection Temperature at 0.46 MPa (66 psi) 55.0 °C131 °FISO 75-2
Vicat Softening Point 116 °C
@Load 1.02 kg
241 °F
@Load 2.25 lb
A50; ISO 306
 
Optical PropertiesMetricEnglishComments
Haze <= 1.5 %<= 1.5 %ASTM D1003
Gloss 135 %135 %20° of arc; ASTM D2457
 
Component Elements PropertiesMetricEnglishComments
SiO2 0.18 %0.18 %Antiblock; Borealis Method

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

Users viewing this material also viewed the following:
Borealis RE239CF Polypropylene Copolymer
Overview of materials for Polypropylene, Extrusion Grade
Kuraray HYBRAR® PH3 Polypropylene Blend
Kuraray HYBRAR® H7125 Hydrogenated Thermoplastic Rubber
Arkema Kynar Flex® 3030-10 PVDF

PBOREA385 / 108644

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.