MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

Melos Mecoline IS RDX 1201 F Irradiation cross-linkable, halogen-free, flame retardant compound
Categories: Polymer; Thermoplastic

Material Notes: Irradiation cross-linkable, halogen-free, flame retardant compound

Compound class: Insulation/Sheathing

Compound category: RDX

Flame retardant: MDH

Standards: DIN/VDE DKE AK 411.2.3; TÜV 2PfG 1169/08.2007

Typical applications: A flame retardant, halogen-free and low smoke, oil resistant compound. Max. operating temperature 125°C

Features: Flame retardant; Halogen-free; Low smoke; Oil resistant; High temperature resistant

Information provided by Melos

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesMetricEnglishComments
Density 1.38 g/cc0.0499 lb/in³pressed plaques; DIN EN ISO 1183-1A
Melt Flow 8.0 g/10 min
@Load 21.6 kg,
Temperature 165 °C
8.0 g/10 min
@Load 47.6 lb,
Temperature 329 °F
DIN EN ISO 1133
 
Mechanical PropertiesMetricEnglishComments
Hardness, Shore D 4545pressed plaques; DIN ISO 7619-1
Tensile Strength 11.5 MPa1670 psiextruded tapes; IEC 60811-501
 18.0 MPa2610 psicross-linked plaques or tapes, 80kGy; IEC 60811-501
 9.304 MPa
@Temperature 100 °C,
Time 86400 sec
1349 psi
@Temperature 212 °F,
Time 24.0 hour
extruded tapes, Fluid IRM 902; IEC 60811-404
 9.77 MPa
@Temperature 23.0 °C,
Time 605000 sec
1420 psi
@Temperature 73.4 °F,
Time 168 hour
extruded tapes, 1N Oxalic acid; IEC 60811-404
 10.478 MPa
@Temperature 23.0 °C,
Time 605000 sec
1519.7 psi
@Temperature 73.4 °F,
Time 168 hour
extruded tapes, 1N NaOH; IEC 60811-404
 12.18 MPa
@Temperature 180 °C,
Time 518000 sec
1767 psi
@Temperature 356 °F,
Time 144 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 12.78 MPa
@Temperature 165 °C,
Time 1.73e+6 sec
1854 psi
@Temperature 329 °F,
Time 480 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 13.8 MPa
@Temperature 155 °C,
Time 3.629e+6 sec
2000 psi
@Temperature 311 °F,
Time 1008 hour
extruded tapes, After ageing in air oven; IEC 60811-401
Elongation at Break 213 %213 %cross-linked plaques or tapes, 80kGy; IEC 60811-501
 229 %229 %extruded tapes; IEC 60811-501
 10 %
@Temperature 200 °C,
Time 900 sec
10 %
@Temperature 392 °F,
Time 0.250 hour
Hot set test, after unloading, 0.2 Mpa; IEC 60811-507
 15 %
@Temperature 250 °C,
Time 900 sec
15 %
@Temperature 482 °F,
Time 0.250 hour
Hot set test, after unloading, 0.2 Mpa; IEC 60811-507
 25 %
@Temperature 200 °C,
Time 900 sec
25 %
@Temperature 392 °F,
Time 0.250 hour
Hot set test, under load, 0.2 MPa; IEC 60811-507
 50 %
@Temperature 250 °C,
Time 900 sec
50 %
@Temperature 482 °F,
Time 0.250 hour
Hot set test, under load, 0.2 MPa; IEC 60811-507
 164.88 %
@Temperature 100 °C,
Time 86400 sec
164.88 %
@Temperature 212 °F,
Time 24.0 hour
extruded tapes, Fluid IRM 902; IEC 60811-404
 171.98 %
@Temperature 165 °C,
Time 1.73e+6 sec
171.98 %
@Temperature 329 °F,
Time 480 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 180.7 %
@Temperature 155 °C,
Time 3.629e+6 sec
180.7 %
@Temperature 311 °F,
Time 1008 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 182.74 %
@Temperature 180 °C,
Time 518000 sec
182.74 %
@Temperature 356 °F,
Time 144 hour
extruded tapes, After ageing in air oven; IEC 60811-401
 254.88 %
@Temperature 23.0 °C,
Time 605000 sec
254.88 %
@Temperature 73.4 °F,
Time 168 hour
extruded tapes, 1N NaOH; IEC 60811-404
 255.8 %
@Temperature 23.0 °C,
Time 605000 sec
255.8 %
@Temperature 73.4 °F,
Time 168 hour
extruded tapes, 1N Oxalic acid; IEC 60811-404
Penetration 8.0
@Temperature 140 °C,
Time 14400 sec
8.0
@Temperature 284 °F,
Time 4.00 hour
[%] Hot pressure test, extruded tapes; IEC 60811-508
 
Electrical PropertiesMetricEnglishComments
Volume Resistivity  6.60e+11 ohm-cm
@Temperature 90.0 °C
6.60e+11 ohm-cm
@Temperature 194 °F
500V; DIN IEC 60093
 3.50e+14 ohm-cm
@Temperature 23.0 °C
3.50e+14 ohm-cm
@Temperature 73.4 °F
500V; DIN IEC 60093
 
Thermal PropertiesMetricEnglishComments
Maximum Service Temperature, Air 125 °C257 °F
Minimum Service Temperature, Air -40.0 °C-40.0 °F
 
Processing PropertiesMetricEnglishComments
Processing Temperature 190 - 200 °C374 - 392 °FMaximum mass temperature
 190 - 210 °C374 - 410 °FTool
Zone 1 140 - 160 °C284 - 320 °F
Zone 2 150 - 170 °C302 - 338 °F
Zone 3 170 - 190 °C338 - 374 °F
Zone 4 175 - 195 °C347 - 383 °F
Zone 5 180 - 200 °C356 - 392 °F
Adapter Temperature 180 - 200 °C356 - 392 °F
Head Temperature 180 - 200 °C356 - 392 °F
Drying Temperature 60.0 - 70.0 °C140 - 158 °F
Dry Time 4.00 - 6.00 hour4.00 - 6.00 hour
Shelf Life 12.0 Month12.0 Month
 
Component Elements PropertiesMetricEnglishComments
Loss on Ignition(%) 30 %30 %pressed plaques; ASTM D 2863 A

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to view all the property values for this datasheet as they were originally entered into MatWeb.

PMELOS021 / 296128

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.