MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Unitika A1030GFL45 PA6, 45% Glass Fiber Reinforced, Conditioned
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 6 (PA6); Nylon 6, 50% Glass Fiber Filled

Material Notes:

Information provided by Unitika Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.50 g/ccISO 1183
Water Absorption 1.0 %
@Time 86400 sec
ISO 62
Moisture Absorption at Equilibrium 1.5 %50% RH; ISO 62
Linear Mold Shrinkage, Flow 0.0010 cm/cm
@Thickness 3.20 mm
Linear Mold Shrinkage, Transverse 0.0030 cm/cm
@Thickness 3.20 mm
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 109ISO 2039
Tensile Strength at Break 150 MPaISO 527-1/-2
Elongation at Break 4.9 %ISO 527-1/-2
Tensile Modulus 8000 MPaISO 527-1/-2
Flexural Strength 220 MPaISO 178
Flexural Modulus 7600 MPaISO 178
Charpy Impact Unnotched 92.0 kJ/m²ISO 179-1
Charpy Impact, Notched 23.0 kJ/m²ISO 179-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 7.00e+11 ohm-cmIEC 60093
Dielectric Strength 1020 V/mil
@Thickness 1.00 mm
IEC 60243-1
Dissipation Factor 0.012
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 550 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear 23.0 µm/m-°CISO 11359-2
Flammability, UL94 HB
@Thickness 0.860 mm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Conditioned)
Niche Polymer POLIXL™ PA6GF40BK PA6, 40% Fiberglass/Mineral Reinforced, Conditioned
BASF Ultramid® A3WG8 BK 20560 40% Glass Filled PA66 (Dry)
BASF Ultramid® B3G8 BK00564 40% Glass Filled PA6 (Dry)
Radici Radiflam® A RV350AF (cond.) Nylon 66-35GF

PUNITIK814 / 177836

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.