MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
CHT Group QM 135 QSI Quantum Silicones 35 Durometer Condensation Cured Moldmaking Material
Categories: Polymer; Thermoset; Silicone

Material Notes: QM 135 is a two-component, room temperature condensation cure silicone material. The cured rubber has excellent mechanical properties and good shelf-life stability. This material is an excellent choice for the molding of intricate patterns, skin molding and applications where high durometer, dimensional stability and extremely tough rubber are required.

Key Features:

  • Low viscosity
  • High tear strength
  • Fast demold time
  • Excellent dimensional stability
Main Applications:
  • Molds for small statues and large statues
  • Molds for polyester, polyurethane and epoxy resin castings
  • Molds for technical articles and prototype
  • Molds for furniture and picture frame replication

      Formerly Amber Chemical Co (ACC Silicones), aquired by CHT in 2017

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.03 g/ccUncatalyzed, QM CAT 135
 1.16 g/cccatalyzed with QM CAT 135
Viscosity 150 cPUncatalyzed, QM CAT 135
 31000 cPcatalyzed with QM CAT 135
 45000 cPBase
Linear Mold Shrinkage <= 0.0030 cm/cmcured 72 hrs @ RT
Storage Temperature <= 38.0 °C6 months
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 35cured 72 hrs @ RT
Tensile Strength 3.40 MPacured 72 hrs @ RT
Elongation at Break 400 %cured 72 hrs @ RT
Tear Strength 150 plicured 72 hrs @ RT
 
Processing PropertiesOriginal ValueComments
Cure Time 12 - 16 hourDemold time, catalyzed with QM CAT 135
Tack-Free Time 4.00 - 6.00 hourCatalyzed with QM CAT 135
 
Descriptive Properties
ColorBeigeBase
 Light Purple catalyzed with QM CAT 135
 PurpleUncatalyzed, QM CAT 135

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Shin-Etsu Silicones KE-541U Silicone Rubber

PACC060 / 22187

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.