MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Special Metals INCOLOY® Alloy 020
Categories: Metal; Superalloy; Iron Base

Material Notes: A nickel-iron-chromium alloy with additions of copper and molybdenum. It also contains niobium for stabilization against sensitization and resultant intergranular corrosion. The alloy has excellent resistance to general corrosion, pitting, and crevice corrosion in chemicals containing chlorides and sulfuric, phosphoric, and nitric acids. Used for tanks, piping, heat exchangers, pumps, valves, and other process equipment. Standard product forms are round, flats, pipe, tube, plate, sheet, strip, and wire.

Data provided by the manufacturer, Special Metals.

Key Words: ASME SB-462 - SB-464, SB-468, Boiler Code Sections III, VIII, IX, UNS N08020; ASTM B 462 - B 464, B 468, B 472 - B 474, B 751
Vendors: Visit metalmen for your metals needs. Products include special chemistry, tight tolerances, custom tempers, odd dimensions/forms, and small quantities. Phone 1-800-767-9494.

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 8.05 g/cc
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 620 MPaAnnealed prior to test
 540 MPa
@Temperature 550 °C
Annealed prior to test
Tensile Strength, Yield 300 MPa
@Strain 0.2 %
Annealed prior to test
 210 MPa
@Strain 0.2 %,
Temperature 550 °C
Annealed prior to test
Elongation at Break 41 %Annealed prior to test.
 40 %
@Temperature 550 °C
Annealed prior to test.
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.000108 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 14.7 µm/m-°C
@Temperature 20.0 - 100 °C
Specific Heat Capacity 0.500 J/g-°C
Thermal Conductivity 12.3 W/m-K
 
Component Elements PropertiesOriginal ValueComments
Carbon, C <= 0.070 %
Chromium, Cr 19 - 21 %
Copper, Cu 3.0 - 4.0 %
Iron, Fe 35 %As remainder
Manganese, Mn <= 2.0 %
Molybdenum, Mo 2.0 - 3.0 %
Nickel, Ni 32 - 38 %
Niobium, Nb (Columbium, Cb) <= 1.0 %Nb min. is 8xC.
Phosphorus, P <= 0.045 %
Silicon, Si <= 1.0 %
Sulfur, S <= 0.035 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
ATI Allvac® Nickelvac® 23 UNS N08020 Specialty Steel
Special Metals INCOLOY® Alloy 800
Carpenter 20Cb-3® Stainless Steel
Carlson 20 Plus Alloy
Special Metals INCOLOY® Alloy 800HT™

NIND01 / 17518

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.