Description DSM Somos® 10120 is a high-speed liquid photopolymer that produces strong, rigid, and durable parts with optical clarity using stereolithography machines. This material is especially useful in applications requiring optical clarity such as fluid flow analysis, stress analysis and light pipes. Other applications include those that require a strong and durable product without the brittleness normally associated with a rigid stereolithography resin. Application Somos® 10120 Photopolymer is used in the solid imaging process to build three-dimensional parts. Somos® 10120 requires a minimal post-cure by UV fluorescent light. Prolonged exposure to UV light will create a yellow tinge to the parts. Information Provided by DSM Desotech Inc. |
Proto3000 provides design tools, 3D printers, additive manufacturing processes, metrology technologies, high-performance materials, and part-finishing automation. Our ISO 9001:2015 additive manufacturing production facility offers 3D printing services, rapid prototyping services, and end-part production with HP MultiJet Fusion (MJF), FDM, SLA, SLS, Polyjet, DLP, metal binder jetting, BMD, and DMLS. Axis Proto Inc. Industry leaders in providing high quality Rapid Prototyping and Additive Manufacturing solutions using all major 3D printing systems including SLA prototyping. Free online quotes at www.axisproto.comClick here to view all available suppliers for this material.Please click here if you are a supplier and would like information on how to add your listing to this material. |