MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Wacker Wacker® L 654 Silicone Fluid
Categories: Fluid; Polymer

Material Notes: Product description: WACKER® L 654 is a solvent-based system containing a reactive polydimethylsiloxane as well as an aminofunctional polydimethylsiloxane. Curing rate and film flexibility can be adapted to special demands by appropriate combination of WACKER® L 654 with non reactive WACKER® L 656.

Application: WACKER® L 654 is used in paint conditioners and paint polishes in order to provide superior gloss and detergent resistance. In comparison with conventional polydimethylsiloxanes of the series WACKER® AK, aminofunctional WACKER® L 654 exhibits an excellent affinity to various substrates. Gloss and depth of color are retained for a longer period of time.

Information provided by Wacker Chemie AG.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 50 %
Kinematic Viscosity 125 cSt
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.4105
Transmission, Visible 90 %"Clear" but manufacturer does not quantify.
 
Descriptive Properties
Amine number0.28
Appearanceclear

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PWACK9787 / 205316

Aluminum Castings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at info@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2025 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.